Patents
US 7,871,946 B2#18468534 Most CitedExpiredUnited States (USPTO)Utility

Nonwoven fabric composed of ultra-fine continuous fibers, and production process and application thereof

6Forward Citations (#18468534 Global)
0.4/yrCitation Velocity (#19861226 Global)
1.41Citation PageRank (#25055481 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A nonwoven fabric composed of ultra-fine continuous fibers having a mean fineness of not more than 0.5 dtex is prepared. The nonwoven fabric comprises a water-soluble thermoplastic resin in a proportion of not more than 5% by weight relative to the nonwoven fabric, has an absorbing height of not less than 30 mm as determined at 20° C. after 10 minutes based on Byreck method when the nonwoven fabric immersion-treated for 60 minutes in a water of 80° C. is used, and satisfies the following formula: (B)/(A)≧0.25, wherein the symbol (B) represents a tensile strength [N/5 cm] in the longitudinal direction and the lateral direction of the nonwoven fabric and the symbol (A) represents a fabric weight [g/m] of the nonwoven fabric. In the nonwoven fabric, not less than 30% of the surface may be coated with the water-soluble thermoplastic resin. The water-soluble thermoplastic resin may be a water-soluble thermoplastic polyvinyl alcohol, e.g., a modified polyvinyl alcohol containing an ethylene unit in a proportion of 3 to 20 mol %. The present invention provides a nonwoven fabric composed of ultra-fine continuous fibers, having a high flexibility or softness, and having a high mechanical st

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A nonwoven fabric comprising: ultra-fine continuous fibers of a water-insoluble thermoplastic resin having a mean fineness of not more than 0.5 dtex and a fine crimp; and a water-soluble thermoplastic polyvinyl alcohol in a proportion of 0.03 to 4.0% by weight relative to the nonwoven fabric; wherein not less than 30% of the surface of the nonwoven fabric constitutes the water-soluble thermoplastic polyvinyl alcohol, wherein said nonwoven fabric has an absorbing height of 50 to 300 mm as determined at 20° C. after 10 minutes based on Byreck method when the nonwoven fabric is immersion-treated

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • U.S. Appl. No. 12/442,124, filed Mar. 20, 2009, Tsujimoto, et al.