A process for recovery of silica and alumina from fly ash, in which, Si is leached out from the fly ash in the form of Na 2 SiO 3 using a NaOH solution of NaOH >40% (w/w), followed by separation to obtain a Na 2 SiO 3 solution and a residue having Al—Si ratio ≧2; vaporizing the solution to obtain Na 2 SiO 3 solutions of various concentrations, or producing silica by carbonation, and producing Al 2 O 3 by prior art methods from residues obtained after alkali-leaching, ultimately producing filler or cement from the residue after the recovery of Al. The method permits recovery of Al 2 O 3 directly from fly ash by removing Si before recovering the Al, which raises the Al—Si ratio of the residue after alkali-leaching and thus simplifies the recovery of Al 2 O 3 and raises the rate of Al recovery from fly ash. The invention further includes calcining high Al coal gangue, kaolinite and middle-low-class bauxite at 900-1100° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for recovering silica and alumina from coal fly ash, comprising: a) alkali-leaching Si from fly ash at 70-150° C. with a NaOH solution of concentration >40% (w/w), then separating a Na 2 SiO 3 solution from a residue having Al—Si ratio ≧2; b) concentrating the Na 2 SiO 3 solution by vaporization, or obtaining silica by carbonation; and c) producing Al 2 O 3 from the residue having Al—Si ratio ≧2.

  2. Claim 2Depends on #1

    The process of claim 1 , wherein the fly ash is activated by one or more of the following steps: a) roasting-activating the fly ash, b) steeping fly ash in H 2 SO 4 solution, c) steeping fly ash in NaOH solution.

  3. Claim 3Depends on #1

    The process of claim 1 , wherein the fly ash is a high Al coal gangue, a kaolinite or middle-low-class bauxite and further comprises activating the fly ash at 900-1100° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (2)

  • Blanco et al, variation in fly ash properties with milling and acid leaching, 2005, fuel, 84, pp. 89-96.
  • Lin et al, the complex chemical treatment of alumina-silica-containing materials, 1998, journal of materials synthesis and processing, vol. 6 No. 1.