Semiconductor device with epitaxial C49-titanium silicide (TiSi2) layer and method for fabricating the same
Abstract
The present invention relates to a semiconductor device with an epitaxially grown titanium silicide layer having a phase of C49 and a method for fabricating the same. This titanium silicide layer has a predetermined interfacial energy that does not transform the phase of the titanium layer, and thus, occurrences of agglomeration of the titanium layer and a grooving phenomenon can be prevented. The semiconductor device includes: a silicon layer; an insulation layer formed on the silicon layer, wherein a partial portion of the insulation layer is opened to form a contact hole exposing a partial portion of the silicon layer; an epitaxially grown titanium silicide layer having a phase of C49 and formed on the exposed silicon substrate disposed within the contact hole; and a metal layer formed on an upper surface of the titanium silicide layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 14.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A semiconductor device, comprising: a silicon layer; an insulation layer formed on the silicon layer. wherein a partial portion of the insulation layer is opened to form a contact hole exposing a partial portion of the silicon layer; an epitaxially grown titanium silicide layer having a phase of C49 and formed on the exposed silicon substrate disposed within the contact hole; and a metal layer formed on an upper surface of the titanium silicide layer, wherein the silicon layer and the titanium silicide layer have an orientation relationship as: (060) [001]TiSi 2 //(002) [110]Si.
- Claim 2Depends on #1
The semiconductor device as recited in claim 1 , wherein the metal layer includes a titanium nitride barrier layer at a region contacting the titanium silicide layer to prevent diffusions of atoms between the metal layer and the silicon layer.
- Claim 3Independent Claim
The
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (5)
- "Crystallographic Structures and Parasitic Resistances of Self-Aligned Silicide TiSi2/Self-Aligned Nitrided Barrier Layer/Selective Chemical Vapor Deposited Aluminum in Fully Self-Aligned Metallization Metal Oxide Semiconductor Field-Effect Transistor" by Chang-Hun Lee, et al.; Jpn. J. Appl. Phys. v
- "Epitaxial Growth of TiSi2 (C49) on (001) Si by Rapid Thermal Annealing" LiMing Wang et al., Oct. 1997, Jpn. J. Appl. Phys. vol. 36 pp. 6475-6480.
- Byun, J.S., "Epitaxial C49-TiSi2 Formation on (100)Si Substrate Using TiNx and Its Electrical Characteristics as a Shallow Contact Metallization," J. Electrochem. Soc., Jun. 1996, pp. 1984-1991, vol. 143(6).
- Office Action for German Patent Application 10361829.5-33 dated Mar. 5, 2008 (6 pages).
- SM SZE, "VLSI Technology", McGraw-Hill, 2nd Edition, (1984), pp. 15, 466 & 486.