US 7,867,600 B2#43830147 Most CitedExpiredUnited States (USPTO)Utility

Deodorant suede-tone-leather-like sheet

2Forward Citations (#43830147 Global)
0.1/yrCitation Velocity (#41849779 Global)
0.92Citation PageRank (#46516338 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A suede-type leather-like sheet having excellent appearance and exhibiting an excellent deodorizing effect and a soft feel in combination without agglomeration of napped fibers or deterioration in the appearance (whitening) due to the deodorant is provided. The deodorant suede-type leather-like sheet comprises a fiber-entangled fabric comprising a microfine fiber and a particulate deodorant, wherein the surface area of the microfine fiber per the unit volume of the fiber-entangled fabric is 3×10 3 to 9×10 4 cm 2 /cm 3 , and at least a portion of the deodorant having an average diameter of primary particles of 0.1 μm or smaller is present on the surface of the microfine fiber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An artificial suede sheet having deodorant properties comprising a fiber-entangled fabric, wherein: the fiber-entangled fabric comprises at least one microfine fiber and a particulate deodorant; a surface area of the at least one microfine fiber per unit volume of the fiber-entangled fabric is from 3×10 3 cm 2 /cm 3 to 9×10 4 cm 2 /cm 3 ; at least a portion of the particulate deodorant is present on a surface of the at least one microfine fiber; and the particulate deodorant comprises particles having an average primary particle diameter of 0.1 μm or less.

  2. Claim 2Depends on #1

    The sheet according to claim 1 , further comprising an elastic polymer, wherein: the elastic polymer is impregnated into the fiber-entangled fabric; and the elastic polymer is present in an amount of from 0 to 150% by mass relative to a total mass of the fiber entangled fabric.