Patents
US 7,867,313 B2#22254557 Most CitedActiveUnited States (USPTO)Utility

Porous β-SiC-containing ceramic molded article comprising an aluminum oxide coating, and method for the production thereof

5Forward Citations (#22254557 Global)
0.3/yrCitation Velocity (#23222717 Global)
1.21Citation PageRank (#31775796 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention concerns a process for the production of a porous β-SiC-bearing ceramic molded body that includes an aluminum oxide layer at the surface of the pores and passages of the porous β-SiC-bearing ceramic molded body. The invention further concerns a porous β-SiC-bearing ceramic molded body which has pores of a mean pore size in the range of between 0.1 urn and 50 μm and an aluminum oxide layer at the surface of the open pores and passages.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the production of a porous β-SiC-bearing ceramic molded body having a three-dimensional continuous β-SiC-structure, which has substantially no grain boundaries, the process including the steps of: (a) extruding a molded body from a material which includes silicon-bearing particles, carbon-bearing particles, aluminum-bearing particles and a cokable organic binding agent, (b) pyrolyzing the porous molded body produced in step (a) at a temperature of between 600 and 1000° C., (c) silicating the porous molded body by heating to a temperature in a range of between 1100 and 1500° C. to

  2. Claim 2Depends on #1

    The process as set forth in claim 1 , wherein the aluminu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,481,179 AMethod for forming fibrous silicon carbide insulating material198439
US 4,514,346 AMethod of making thermal-shock resistant molded articles on the basis of silicon carbide198540
US 4,564,496 AMethod of making porous silicon carbide bodies198635
US 4,777,152 APorous silicon carbide sinter and its production198887
DE 3,719,606 A1Verfahren zur silicierung von poroesen formkoerpern aus siliciumcarbid oder siliciumcarbid/kohlenstoff—6
EP 4,025,239 A1Therapeutic fusion proteins—0
WO 9,313,303 A1A filter unit and a filter body for filtering exhaust gas from diesel engines—36
EP 0,570,847 A1Sorption of organic compounds from gases—12
US 5,324,692 AProcess for producing moldings from silicon-infiltrated silicon carbide199416
US 5,389,325 AActivated carbon bodies having phenolic resin binder199564
DE 4,339,667 A1Energiesparendes Verfahren zur Sorption von organischen Verbindungen aus Gasen—5
EP 0,657,403 A1Porous ceramic and process for producing the same—8
US 5,429,782 AProcess for producing polytetrafluoroethylene molded article199525
US 5,451,554 AActivated carbon bodies having epoxy resin and bentonite binders199515
DE 4,413,127 C1Verfahren zur Herstellung poröser, durchströmbarer Formkörper aus Siliciumcarbid und Formkörper199512
US 5,474,587 APorous fluid-permeable moldings of silicon carbide and process of production199530
US 5,488,021 AActivated carbon bodies having clay binder and method of making same199653
US 5,538,681 ADrying process to produce crack-free bodies199657
US 5,543,096 AMethod for producing activated carbon bodies having silicone resin binder199630
EP 0,796,830 A1Porous permeable body and method for its preparation—14
DE 19,727,115 A1Porous silicon carbide ceramic production—17
US 5,759,460 ACeramic porous bodies and method of producing the same19988
DE 19,711,831 A1Schmelzinfiltrierte faserverstärkte Verbundkeramik—30
US 5,853,444 APorous permeable molded body199846
US 5,914,294 AAdsorptive monolith including activated carbon and method for making said monlith1999154

Non-Patent Literature (5)

  • Brunauer et al., "Adsorption of gases in multimolecular layers", J. Am. Chem. Soc., 1938, 309, vol. 60.
  • Ferro et al., "Wetting behavior in the Al-Si/SiC system: Interface reactions and solubility effects", Acta metall. Mater., 1995, 3061-3073, vol. 43(8).
  • Fitzner et al., "Fiber-Reinforced Silicon Carbide", Am. Cer. Soc. Bull., 1986, 326, vol. 65.
  • Greil et al., "Effect of microstructure on the fracture behavior of biomorphous silicon carbide ceramics", Journal of the European Ceramic Society, 2002, 2697-2707, vol. 22(14-15).
  • Greil et al., Biomorphic Cellular Silicon Carbide Ceramics from Wood: I. Processing and Microstructure, J. Eur. Ceram. Soc., 1998, 1961-1973, vol. 18.