Patents
US 7,863,386 B2#33923172 Most CitedActiveUnited States (USPTO)Utility

Low density ethylenic polymer composition and method of making the same

3Forward Citations (#33923172 Global)
0.2/yrCitation Velocity (#33266194 Global)
0.98Citation PageRank (#42752847 Global)
15Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The instant invention is an improved low-density ethylenic polymer composition and method of making the same. The polymer composition according to instant invention includes a major component, and a minor component. The major component is an LDPE resin having a melt index (I 2 ) in the range of about 0.01 dg/min to about 100 dg/min, a M W(abs) /M W(GPC) ratio of about 2.6 or less, and a melt strength of less than (14.0 e (−1.05 * log 10(MI)) )cN Jj16 mmor component is an LDPE resin having a melt index (I 2 ) of less than about 5 dg/min, a molecular weight distribution of greater than about 7, and a M W(abs) /M W(GPC) ratio of at least 2.7. The polymer composition of the instant invention may further include additional components.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A composition comprising: a major component, wherein said major component comprising a high pressure highly branched LDPE resin having a melt index (MI) tested at 190° C. ASTM D1238: 2.16 kg weight dg/minute in the range of about 0.01 dg/min to about 100 dg/min, a M w(abs) /M w(GPC) ratio of about 2.6 or less, and a melt strength of less than (14.0 e (−1.05 * log 10(MI)) )) cN; and a minor component, wherein said minor component comprising a high pressure highly branched LDPE resin having a melt index (MI) tested at 190° C. ASTM D1238: 2.16 kg weight dg/minute of less than about 5 dg/min, a m

  2. Claim 2Depends on #1

    The composition according to claim 1 , wherein said minor component having a melt index (MI) tested at 190° C. ASTM D1238: 2.16 kg weight dg/

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Balke, Stephen T., et al., A Strategy for Interpreting Multidetector Size-Exclusion Chromatography Data II, Chromatography of Polymers, 1993, pp. 199-219.
  • Hawley's Condensed Chemical Cictionary, 14th edition (2002).
  • Kratochvil, P., Polyethylene, Classical Light Scattering from Polymer Solutions, 1987, pp. 302-307, Chpt. 7, Elsevier, New York.
  • Kratochvil, P., Some Other Applications of Light Scattering, Classical Light Scattering from Polymer Solutions, 1987, pp. 237-255, Chpt. 6, Elsevier, New York.
  • Mourey, Thomas H., et al., A Stratefy for Interpreting Multidetector Size-Exclusion Chromatography Data I, Chromatography of Polymers, 1993, pp. 180-198.