US 7,862,896 B2#11586415 Most CitedActiveUnited States (USPTO)Utility

Core-shell resin particle having low content of volatile components, and resin dispersion

9Forward Citations (#11586415 Global)
0.6/yrCitation Velocity (#13035929 Global)
2.13Citation PageRank (#13098468 Global)
18Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to core-shell resin particles (C2) each comprising one or more film-like shell layers (P) comprising a first resin (a) and a core layer (Q) comprising a second resin (b). The core-shell resin particle (C2) is characterized in that the weight ratio between (P) and (Q) is from 0.1:99.9 to 70:30, the volatile content in the resin particle (C2) is not more than 2 weight %, and the resin (a) has an initial softening temperature of 40 to 270° C., a Tg of 20 to 250° C., a flow temperature of 60 to 300° C., and the difference of the Tg and the flow temperature in a range of 0 to 120° C. The resin particles are excellent in electrostatic property, thermal storage stability and thermal properties, and exhibit a narrow particle diameter distribution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 9.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Core-shell type resin particles (C2) each comprising a film shell layer (P) in one or more layer structure made of a first resin (a) and a core layer (Q) in one layer structure made of a second resin (b), wherein the weight ratio of the film shell layer (P) and the core layer (Q) is in a range of (0.1:99.9) to (70:30), the content of volatile components of the resin particles (C2) is 2% by weight or lower, and the resin (a) has an initial softening temperature of 40 to 270° C., a glass transition temperature of 20 to 100° C., a flow temperature 60 to 220° C., and the difference of the glass tr

  2. Claim 2Depends on #1

    The resin particles according to claim 1 , wherein the resin (a) is at least one resin selected from polyester resins, epoxy resins, and vinyl resins.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Japanese Office Action dated Oct. 20, 2009, in corresponding Japanese Patent Application No. 2005-024598.
  • Japanese Patent Office Action in corresponding application JP2005-024598, mailed May 27, 2008 (with English Summary).
  • Japanese Patent Office Action in corresponding application JP2005-024613, mailed Aug. 21, 2007 (with English Summary).
  • Japanese Patent Office Action in corresponding application JP2005-024613, mailed Feb. 26, 2008 (with English Summary).
  • Japanese Patent Office Action in corresponding application JP2005-024613, mailed Nov. 20, 2007 (with English Summary).