Build-up wear-resistant copper alloy and valve seat

6Forward Citations (#18597118 Global)
0.4/yrCitation Velocity (#21241972 Global)
1.37Citation PageRank (#26368238 Global)
18Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

While securing the building-up ability and crack resistance, to provide a build-up wear-resistant copper alloy and valve seat. The build-up wear-resistant copper alloy and valve seat are characterized by having a composition of nickel: 5.0-24.5%, iron: 3.0-20.0%, silicon: 0.5-5.0%, boron: 0.05-0.5%, chromium: 0.3-5.0%, one member or two members or more selected from the group consisting of molybdenum, tungsten and vanadium: 3.0-20.0%, by weight %, and the balance being copper and inevitable impurities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 6.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A build-up wear-resistant copper alloy, consisting of:

  2. Claim 5Independent Claim

    0-24.5% Ni, 3.0-20.0% Fe, 0.5-5.0% Si, 0.05-0.3% B, 0.3-5.0% Cr, 0.01-2.0% Co, an element selected from the group consisting of molybdenum, tungsten, vanadium, and a mixture thereof in an amount of 3.0-20.0%, by weight %, and a balance being copper and inevitable impurities, wherein a ratio of an amount of Cr to an amount of B is four or more.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Tanaka et al., "Development of Laser Clad Valve Seat Alloys," Toyota Chuo Kenkyusho R&D Rebyu, X, XX, vol. 28, No. 3, pp. 35-45, Sep. 1, 1993.