Ferritic ductile cast iron alloys having high carbon content, high silicon content, low nickel content and formed without annealing
Abstract
Disclosed are methods of making ferritic ductile iron castings (60-40-18) with high toughness (6 ft.lb minimum Charpy V at −20 F and 10 ft.lb minimum Charpy V at +72 F), without adding Nickel and without annealing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A cast iron alloy having: a toughness of at least 6 ft. lb Charpy V at −20° F. and a toughness of at least 10 ft. lb Charpy V at +72° F.; a tensile strength of at least 60,000 psi; a yield strength of at least 40,000 psi; and an elongation of at least 18%; the alloy comprising: (a) 3.30-3.85% Carbon by mass; (b) 2.35-2.90% Silicon by mass; (c) 0.020-0.060% nodularizing agent by mass; (d) 0-0.40% Manganese by mass; (e) 0-0.15% Copper by mass; (f) 0-0.10% Chromium by mass; (g) 0-0.050% Phosphorus by mass; (h) 0-0.030% Sulfur by mass; (i) 0-0.25% Nickel by mass; (j) 0-0.10% any other incidental n
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 9,945,003 B2 | Impact resistant ductile iron castings | 2018 | 0 |
References Cited — Backward Prior Art (30)
Non-Patent Literature (4)
- Cesar Braga; Sorelmetal®; Ductile Iron Data for Design Engineers; Published by Rio Tinto Iron & Titanium, a member of the Ductile Iron Marketing Group; Revised/Reprinted 1998.
- Ductile Iron Bomb Bodies; http://www.ductile.org/magazine/1998-3/bomb.htm; Jun. 1, 2007.
- Ductile Iron Bomb Bodies; http://www.ductile.org/magazine/1998—3/bomb.htm; Jun. 1, 2007.
- Ductile Iron DCI (A395), Flowserve Corporation, May 1999.