Abstract

The present invention relates to technology for manufacturing electrical steel sheets having excellent magnetic properties through the control of a hot-rolled texture using the phase transformation of steel. More particularly, it relates to a non-oriented electrical steel sheet that has reduced iron loss and increased magnetic flux density by controlling alloy component elements and optimizing hot-rolling conditions, even though hot-rolled sheet annealing is not carried out, as well as a manufacturing method thereof. More specifically, the invention provides a non-oriented electrical steel sheet which has excellent magnetic properties while hot-rolled sheet annealing can be omitted, the steel sheet being comprised of 0.005 wt % or less of C, 1.0-3.0 w % of Si, 0.1-2.0 wt % of Mn, 0.1 wt % or less of P, 0.1-1.5 wt % of Al, and a remainder of Fe and other inevitable impurities, in which the relationship between the elements Mn and Al satisfies an equation of −0.2<m(=Mn−Al)<1.0, and a slab for the steel sheet, when reheated, has a two-phase region of austenite+ferrite at a temperature ranging from ArI to 1250° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a non-oriented electrical steel sheet that has excellent magnetic properties while hot-rolled sheet annealing can be omitted, the method comprising the steps of: reheating a slab comprising 0.005 wt % or less of C, 1.0-3.0 wt % of Si, 0.1-2.0 wt % of Mn, 0.1 wt % or less of P, 0.1-1.5 wt % of Al, wherein the elements Mn and Al satisfy an equation of −0.2<Mn−Al<1.0 and a remainder of Fe and other inevitable impurities, to a temperature ranging from Ar1 to 1250° C.; hot-rolling the reheated slab in such a manner that 70% or more of a total hot finish rolling is p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • English-language abstract of Japanese Patent Publication No. JP 07-097628, published Apr. 11, 1995, esp@cenet database.
  • English-language abstract of Korean Patent Publication No. KR 10-2003-0052139, published Jun. 26, 2003, esp@cenet database.