Method for manufacturing semiconductor device using quadruple-layer laminate
Abstract
There is provided a laminate used as an underlayer layer for a photoresist in a lithography process of a semiconductor device and a method for manufacturing a semiconductor device by using the laminate. The method comprising: laminating each layer of an organic underlayer film (layer A), a silicon-containing hard mask (layer B), an organic antireflective film (layer C) and a photoresist film (layer D) in this order on a semiconductor substrate. The method also comprises: forming a resist pattern in the photoresist film (layer D); etching the organic antireflective film (layer C) with the resist pattern; etching the silicon-containing hard mask (layer B) with the patterned organic antireflective film (layer C); etching the organic underlayer film (layer A) with the patterned silicon-containing hard mask (layer B); and processing the semiconductor substrate with the patterned organic underlayer film (layer A).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 6.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
The method for manufacturing a semiconductor device comprising: laminating each layer of an organic underlayer film (layer A), a silicon-containing hard mask (layer B), an organic antireflective film (layer C) and a photoresist film (layer D) in this order on a semiconductor substrate, wherein the organic underlayer film (layer A) is a layer including a polymer having an aromatic condensed ring in a main chain or a side chain bonded to the main chain.
- Claim 2Depends on #1
The method for manufacturing a semiconductor device according to claim 1 , wherein the organic underlayer film (layer A) has a film thickness of 50 to 500 nm; the silicon-containing hard mask (layer B) has a film thickness of 50 to 200 nm; the organic antireflective film (layer C) has a film thickness of 10 to 100 nm; and a film thickness ratio of layer A:layer B:layer C is 1 to 10:1 to 5:1.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (41)
Non-Patent Literature (4)
- Crawford et al., "New Materials for 157 nm Photoresists: Characterization and Properties," Proceedings of SPIE, 2000, pp. 357-364, vol. 3999.
- Patterson et al., "Polymers for 157 nm Photoresist Applications: A Progress Report," Proceedings of SPIE, 2000, pp. 365-374, vol. 3999.
- Schmaljohann et al., "Design Strategies for 157 nm Single-Layer Photoresists: Lithographic Evaluation of a Poly (alpha-trifluoromethyl vinyl alcohol) Copolymer," Proceedings of SPIE, 2000, pp. 330-334, vol. 3999.
- Schmaljohann et al., "Design Strategies for 157 nm Single-Layer Photoresists: Lithographic Evaluation of a Poly (α-trifluoromethyl vinyl alcohol) Copolymer," Proceedings of SPIE, 2000, pp. 330-334, vol. 3999.