A Polyacrylate having an at least bimodal molecular weight distribution is disclosed. The polyacrylate is characterized by at least two maxima in the molar mass distribution curve, at points M 1 and M 2 , with M 1 >M 2 , in which, viewed formally, there are at least two polymers, P 1 and P 2 , each having its own molecular weight distribution, the polymer P 1 possessing a most frequent molar mass M max (P 1 ) and the polymer P 2 possessing a most frequent molar mass M max (P 2 ), where M max (P 1 )>M max (P 2 ), at least the polymer P 1 being based on a monomer mixture comprising at least one monomer type selected from the group of the acrylic esters and of the methacrylic esters of the general formula H 2 C═CR 1 —COOR 2 where R 1 ═H or CH 3 and where R 2 represents an aliphatic hydrocarbon chain having 4 to 15 carbon atoms; and at least one olefinically unsaturated monomer type containing functional groups, wherein the functional groups of the at least one olefinically unsaturated monomer type are groups which are able to react for a thermal crosslinking reaction, and at least the polymer P 1 has copolymerized monomers of the olefinically unsaturated monomer type containing

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Polyacrylate having an at least bimodal molecular weight distribution, characterized by at least two maxima in the molar mass distribution curve, at points M 1 and M 2 , with M 1 >M 2 , in which there are at least two polymers, P 1 and P 2 , each having their own molecular weight distribution, the polymer P 1 having a weight-average molecular weight in the range of from about 800,000 g/mol to 2,000,000 g/mol, and a polydispersity of between 4 to 15 and possessing a most frequent molar mass M max (P 1 ) and the polymer P 2 having a weight-average molecular weight in the range of from abo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Bull. Jam. Phys. Soc. vol. 1, 1956, p. 123.
  • J.O. Metzger: Herstellung (Erzeugung) von Radiklaen durch homolytische Spaltung von C, H-Bindungen mit Radikalen; A. Herstellung, pp. 60-146.