US 7,838,422 B2#63809811 Most CitedActiveUnited States (USPTO)Utility

Al-doped charge trap layer, non-volatile memory device and methods of fabricating the same

0Forward Citations (#63809811 Global)
0.0/yrCitation Velocity (#63809811 Global)
0.56Citation PageRank (#63809811 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided is an aluminum (Al) doped charge trap layer, a non-volatile memory device and methods of fabricating the same. The charge trap layer may include a plurality of silicon nano dots that trap charges and a silicon oxide layer that covers the silicon nano dots, wherein the charge trap layer is doped with aluminum (Al). The non-volatile memory device may include a substrate including a source and a drain on separate regions of the substrate, a tunneling film on the substrate contacting the source and the drain, the charge trap layer according to example embodiments, a blocking film on the charge trap layer, and a gate electrode on the blocking film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a charge trap layer structure comprising: forming an amorphous silicon film on a tunneling film; forming a charge trap layer having a plurality of silicon nano dots and a silicon oxide layer covering the silicon nano dots by partially oxidizing the amorphous silicon film; and doping the charge trap layer with aluminum (Al) at a concentration of about 0.1 to about 10 atom %.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein forming the amorphous silicon film includes depositing the amorphous silicon film to a thickness of about 1 nm to about 5 nm.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein forming the charge trap layer includes annealing the amorphous silicon film at a temperature of about 800° C. to about 900° C. for about 2 minutes to about 3 minutes under a gas atmosphere of about 90% N2 and about 10% O2.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗