Patents
US 7,824,929 B2#110832195 Most CitedActiveUnited States (USPTO)Utility

Method for producing group III nitride-based compound semiconductor

0Forward Citations (#110832195 Global)
0.0/yrCitation Velocity (#110832195 Global)
0.56Citation PageRank (#110832195 Global)
11Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to remove micro-scratches on a surface of a GaN substrate cut from a GaN ingot. The invention is directed to establish a method for surface treatment of a GaN substrate, including heating the surface in an atmosphere containing trimethylgallium, ammonia, and hydrogen. It is preferable that the trimethylgallium feeding rate is 150 μmol/min or higher, the ratio of trimethylgallium feeding rate to ammonia feeding rate (V/III ratio) is 1,200 to 4,000, and the heating temperature is 1,000° C. to 1,250° C. In addition, the temperature of the surface treatment is set to be higher than that of the following GaN growth, and the feed rate of trimethylgallium is lower than that of the growth procedure. RMS of roughness on the substrate was equal to or less than 1.3 nm, and the substrate whose step condition is excellent can be obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing Group III nitride-based compound semiconductor products comprising: performing a surface treatment of a Group III nitride-based compound semiconductor substrate, whose surface having been polished, in an atmosphere containing a Group III element source precursor, ammonia, and hydrogen during heating in order to make the surface of the semiconductor substrate smooth, and epitaxially growing a Group III nitride-based compound semiconductor on the treated surface.

  2. Claim 2Depends on #1

    A method for producing Group III nitride-based compound semiconductor products according to claim 1 , wherein the surface treatment is performed under the conditions which realize a near equilibrium state in which the rate of growth and the rate of decomposition of a Group III nitride are nearly equal.

  3. Claim 3Independent Claim

    A method for producing Group III nitride-based compo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • Chinese Office Action dated May 11, 2010, with English translation.