Method of forming a Schottky diode and structure therefor
Abstract
In one embodiment, a Schottky diode is formed on a doped region having a thickness less than about eighteen microns.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming a Schottky diode comprising: providing a semiconductor substrate having a first surface; forming a first doped region extending into the semiconductor substrate from the first surface and having a resistivity no greater than about two ohm-cm; forming a second doped region within the first doped region and extending less than first distance into the semiconductor substrate; forming a Schottky barrier material contacting the first doped region; forming a dielectric layer on the first surface and extending to overlie the second doped region and have a side substantially coplan
- Claim 2Independent Claim
The metho
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
Non-Patent Literature (2)
- Data Sheet: "NCP1205 Single Ended PWM Controller Featuring QR Operation and Soft Frequency Foldback", © Semiconductor Components Industries, LLC, Oct. 2005, 2005-Rev. 6, 17pps.
- Data Sheet: “NCP1205 Single Ended PWM Controller Featuring QR Operation and Soft Frequency Foldback”, © Semiconductor Components Industries, LLC, Oct. 2005, 2005—Rev. 6, 17pps.