Abstract

At least one basic precipitant selected from the group consisting of NaOH, KOH, NH 4 OH, NH 3 , NH 4 HCO 3 and (NH 4 ) 2 CO 3 is added to an indium salt solution, which contains 0.1 to 3 M of indium, in an adding time of not longer than 24 hours, while the solution is maintained at a temperature of 5 to 95° C. until the equivalent of the basic precipitant reaches an equivalent of 0.5 to 3. Then, a precipitate obtained from the solution by a solid-liquid separation is dried and calcined at a temperature of 570 to 780° C. in an non-oxidizing atmosphere which contains ammonia gas and water vapor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing an indium oxide powder, the method comprising the steps of: adding a basic precipitant to an indium salt solution to produce a precipitate; separating the precipitate by a solid-liquid separation; drying the separated precipitate; and calcining the dried precipitate in an inert gas atmosphere which contains a reducing gas and water vapor, wherein the concentration of indium in said indium salt solution is in the range of from 0.01 M to 3 M, and said basic precipitant is added to said indium salt solution in an amount of 0.5 to 3 equivalents per equivalent of the indium s

  2. Claim 2Independent Claim

    A method for producing an indium oxide powder