Patents
US 7,807,219 B2#62056426 Most CitedActiveUnited States (USPTO)Utility

Repairing and restoring strength of etch-damaged low-k dielectric materials

1Forward Citations (#62056426 Global)
0.1/yrCitation Velocity (#53062307 Global)
0.74Citation PageRank (#62056426 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process of repairing a plasma etched low-k dielectric material having surface-bound silanol groups includes exposing at least one surface of the dielectric material to (a) a catalyst so as to form hydrogen bonds between the catalyst and the surface-bound silanol groups obtaining a catalytic intermediary that reacts with the silane capping agent so as to form surface-bound silane compounds, or (b) a solution comprising a supercritical solvent, a catalyst, and a silane capping agent so as to form hydrogen bonds between a catalyst and the surface-bound silanol groups obtaining a catalytic intermediary that reacts with the silane capping agent so as to form surface-bound silane compounds. Horizontal networks can be formed between adjacent surface-bound silane compounds. The dielectric material can be further treated with an organic acid so as to catalyze a hydrolytic reaction with alkoxy groups on the surface-bound silane compounds forming silanol groups that can be condensed via heat to remove water as a byproduct.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process of repairing a plasma etched low-k dielectric material having surface-bound silanol groups, comprising: (a) exposing at least one surface of the dielectric material to a catalyst so as to form hydrogen bonds between the catalyst and the surface-bound silanol groups thereby obtaining a catalytic intermediary; (b) treating the dielectric material with a silane capping agent such that the silane capping agent reacts with the catalytic intermediary and forms surface-bound silane compounds having at least one alkoxy group; and (c) reacting the at least one alkoxy group on the surface-boun

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,238,899 AActive carbon for deodorization and process for preparation thereof199318
EP 0,675,128 A1Method for preparation of stable water-borne silane compositions—68
US 5,849,369 AMethod for manufacturing a chemically adsorbed film and a chemical adsorbent solution for the method199835
US 2001009894 A1Combination surfactant systems for use in carbon dioxide-based cleaning formulations—2
US 6,277,203 B1Method and apparatus for cleaning low K dielectric and metal wafer surfaces200141
US 6,287,633 B1Finishing agents and method of using the same20016
US 6,297,206 B2Combination surfactant systems for use in carbon dioxide-based cleaning formulations200115
US 6,323,121 B1Fully dry post-via-etch cleaning method for a damascene process2001200
US 6,337,277 B1Clean chemistry low-k organic polymer etch200249
US 2002045347 A1Divided pressure vessel apparatus for carbon dioxide based systems and methods of using same—11
US 6,457,477 B1Method of cleaning a copper/porous low-k dual damascene etch200230
US 6,486,078 B1Super critical drying of low k materials200237
US 6,531,224 B1Self-assembled monolayer and method of making200341
US 6,561,220 B2Apparatus and method for increasing throughput in fluid processing200312
US 6,602,351 B2Methods for the control of contaminants following carbon dioxide cleaning of microelectronic structures200339
US 6,620,733 B2Use of hydrocarbon addition for the elimination of micromasking during etching of organic low-k dielectrics200321
US 2003198895 A1Method of passivating of low dielectric materials in wafer processing—57
US 6,669,785 B2Methods and compositions for etch cleaning microelectronic substrates in carbon dioxide200349
US 2004045588 A1Methods and compositions for etch cleaning microelectronic substrates in carbon dioxide—23
US 6,733,835 B2Self-assembled monolayer and method of making200418
US 6,736,149 B2Method and apparatus for supercritical processing of multiple workpieces200420
US 2004102042 A1Divided pressure vessel apparatus for carbon dioxide based systems and methods of using same—4
US 6,753,038 B2Self-assembled monolayer and method of making200418
US 2004146636 A1Method of coating microelectronic substrates—12
US 6,777,344 B2Post-etch photoresist strip with O2 and NH3 for organosilicate glass low-K dielectric etch applications200425
US 2004187894 A1Wafer clamping apparatus and method for operating the same—7
US 2004187899 A1Chamber for wafer cleaning and method for making the same—7
US 2004187792 A1Chamber for high-pressure wafer processing and method for making the same—27
US 6,841,483 B2Unique process chemistry for etching organic low-k materials200519

Non-Patent Literature (5)

  • Barry Arkles, "Cyclic Azasilanes," Gelest Silane Coupling Agents: Connecting Across Boundaries, v2.0, 2006, p. 13.
  • Barry Arkles, "Hydrolysis Considerations," Gelest Silane Coupling Agents: Connecting Across Boundaries, v2.0, 2006, p. 3.
  • Chinese Official Action dated Jan. 29, 2010 for Chinese Appln. No. 200780024505.X.
  • International Preliminary Report on Patentability issued Jan. 6, 2009 for PCT/US2007/014435.
  • International Search Report and Written Opinion dated Nov. 19, 2007 for PCT/US07/14435.