Abstract

A process for manufacturing a metalloaluminophosphate molecular sieve, the process comprising the steps of: (a) combining at least one silicon source, at least one metal source, at least one structure-directing-agent (R), at least one phosphorus source, and at least one aluminum source to form a mixture having a molar composition according to formula: (n)Si:Al 2 :(m)P:(x)R:(y)H 2 O:(z)M wherein n is in the range of from about 0.005 to about 0.6, m is in the range of from about 1.2 to about 2.4, x is in the range of from about 0.5 to about 2, y is in the range of from about 10 to about 60, and z is in the range of from about 0.001 to 1; and (b) submitting the mixture to crystallization conditions to form the metalloaluminophosphate molecular sieve, wherein the metalloaluminophosphate molecular sieve has an X-ray diffraction pattern having a FWHM greater than 0.10 degree (2θ) and an AEI/CHA framework type ratio of from about 0/100 to about 40/60 as determined by DIFFaX analysis.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a metalloaluminophosphate molecular sieve, said process comprising the steps of: (a) combining at least one silicon source, at least one metal source, at least one structure-directing-agent (R), at least one phosphorus source, and at least one aluminum source to form a mixture having a molar composition according to formula (XII): (n)Si:Al 2 :(m)P:(x)R:(y)H 2 O:(z)M  (XII) wherein n is in the range of from about 0.005 to about 0.6, m is in the range of from about 1.2 to about 2.4, x is in the range of from about 0.5 to about 2, y is in the range of from about 10 to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (5)

  • A.M. Prakesh et al., "Synthesis of SAPO-34: High Silicon Incorporation in the Presence of Morpholine as Template," J. Chem. Soc., Faraday Trans., vol. 90(15), pp. 2291-2296, 1994.
  • Ashtekar et al, "Small Pore Aluminum Phosphate Molecular Sieves with Chabazite Structure: . . . " J. Phys. Chem. (1996), 100, 3665-3670.
  • J. Chen et al., "Understanding the Bronsted Acidity of SAPO-5, SAPO-17, SAPO-18 and SAPO-34 and their Catalytic Performance for Methanol Conversion to Hydrocarbons," Zeolites and Related Microporous Materials: State of the Art 1994; Studies in Surface Science and Catalysis, vol. 84, pp. 1731-1738.
  • Jiesheng Chen et al., "SAPO-18 Catalysts and Their Bronsted Acid Sites," J. Phys. Chem., American Chemical Society, vol. 98, pp. 10216-10224, 1994.
  • Jiesheng Chen et al., "Silicoaluminophosphate No. eighteen (SAPO-18): a new microporous solid acid catalyst," Catalysis Letters, vol. 28, pp. 241-248, 1994.