US 7,805,976 B2#52660797 Most CitedActiveUnited States (USPTO)Utility

Method for checking surface condition after cleaning

1Forward Citations (#52660797 Global)
0.1/yrCitation Velocity (#52596585 Global)
0.82Citation PageRank (#52660797 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods for inspecting gas turbine component parts for possible distress after hydrogen fluoride cleaning are disclosed. The methods selectively remove a small amount of material for IGA inspection and restore the material using the same procedures as when the parts were manufactured.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for determining corrosion in a component part comprising: choosing an area of the component part for examination; removing a predetermined amount of material from the surface of said area to create a new surface; polishing said new surface to a predetermined depth to create a polished surface; determining corrosion in the component part; said corrosion determining step comprising evaluating corrosion by examining said polished surface; and restoring said polished surface back to original dimensions.

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said removing step comprises removing material from said surface to a depth of about 0.010 to 0.020 inch.

  3. Claim 3Depends on #1

    The method according to claim 1 wherein said polishing step comprises polishing said new surface to remove additional material from said new surface to a depth of about 10 to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (1)

  • European Search Report, dated Jul. 10, 2008.