Patents
US 7,803,665 B2#6968412 Most CitedActiveUnited States (USPTO)Utility

Method for encapsulating a device in a microcavity

14Forward Citations (#6968412 Global)
0.9/yrCitation Velocity (#8189796 Global)
2.41Citation PageRank (#10805233 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Manufacturing a semiconductor device involves forming ( 200 ) a sacrificial layer where a micro cavity is to be located, forming ( 210 ) a metal layer of thickness greater than 1 micron over the sacrificial layer, forming ( 220 ) a porous layer from the metal layer, the porous layer having pores of length greater than ten times their breadth, and having a breadth in the range 10 nm-500 nanometers. The pores can be created by anodising, electrodeposition or dealloying. Then the sacrificial layer can be removed ( 230 ) through the porous layer, to form the micro cavity, and pores can be sealed ( 240 ). Encapsulating MEMS devices with a porous layer can reduce costs by avoiding using photolithography for shaping the access holes since the sacrificial layer is removed through the porous membrane.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 14.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device having the steps of: forming a sacrificial layer where a micro cavity is to be located; forming a metal layer of thickness greater than 1 micron over the sacrificial layer; forming a porous layer from the metal layer, the porous layer having pores of length greater than ten times their breadth, and having a breadth in the range of 10-500 nanometers; wherein the metal layer comprises an alloy of metals having differing etch rates, and the step of forming the porous layer comprises etching the deposited alloy to remove the metal having the faster

  2. Claim 2Depends on #1

    The method of claim 1 , the etching step comprising any one or more of: electrochemical etching and chemical etching using an

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Prevention of Corrosion in Structural Aluminum Alloys", http://www.public.asu.edu/~karls/Corrosion.html, pp. 1-4.
  • "Prevention of Corrosion in Structural Aluminum Alloys", http://www.public.asu.edu/˜karls/Corrosion.html, pp. 1-4.
  • Das, B. et al., "Porous Silicon PN Junction Light Emitting Diodes", Semicond. Sci. Technol., vol. 14, pp. 988-993 (1999).
  • Denison et al., "The Use of 'Dry' CO2-based Technologies for the Enhanced Fabrication of Microelectronic Devices." American Chemical Society (2004).
  • He, Rihui et al., "Porous Polysilicon Shell Formed by Electrochemical Etching for On-Chip Vacuum Encapsulation," Solid-State Sensor, Actuator and Microsystems Workshop, Hilton Head Island, SC, Jun. 6-10, 2004, at 332-335.