Patents
US 7,799,149 B2#119900861 Most CitedActiveUnited States (USPTO)Utility

Oil country tubular good for expansion in well and manufacturing method thereof

0Forward Citations (#119900861 Global)
0.0/yrCitation Velocity (#119900861 Global)
0.56Citation PageRank (#119900861 Global)
30Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An oil country tubular good for expansion according to the invention is expanded in a well. The oil country tubular good for expansion has a composition containing, in percentage by mass, 0.05% to 0.08% C, at most 0.50% Si, 0.80% to 1.30% Mn, at most 0.030% P, at most 0.020% S, 0.08% to 0.50% Cr, at most 0.01% N, 0.005% to 0.06% Al, at most 0.05% Ti, at most 0.50% Cu, and at most 0.50% Ni, and the balance consisting of Fe and impurities, and a structure having a ferrite ratio of at least 80%. The oil country tubular good for expansion has a yield strength in the range from 276 MPa to 379 MPa and a uniform elongation of at least 16%. Therefore, the oil country tubular good according to the invention has a high pipe expansion characteristic.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 0.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An oil country tubular good for expansion in a well having a composition comprising, in percentage by mass, 0.05% to 0.08% C, at most 0.50% Si, 0.80% to 1.30% Mn, at most 0.030% P, at most 0.020% S, 0.08% to 0.50% Cr, at most 0.01% N, 0.005% to 0.06% Al, at most 0.05% Ti, at most 0.50% Cu, and at most 0.50% Ni, and the balance consisting of Fe and impurities, a quenched and tempered structure comprising a ferrite ratio of at least 80% and a yield strength in the range from 276 MPa to 379 MPa, wherein the oil country tubular good for expansion has a uniform elongation of at least 18%.

  2. Claim 2Independent Claim

    An oil country tubular good for expansion in a well having a composition comprising, in percentage by mass, 0.05% to 0.08% C, at most 0.50% Si, 0.80% to 1.30% Mn, at most 0.030% P, at most 0.020% S, 0.08% to 0.50% Cr, at most 0.01% N, 0.005% to 0.06% Al, at most 0.05% Ti, at most 0.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
US 4,345,952 AMethod for the manufacture of tubes from steel having high ductility at low temperature19824
US 4,354,882 AHigh performance tubulars for critical oil country applications and process for their preparation198241
JP S58157948 ASteel material with superior resistance to cracking due to hydrogen embrittlement—8
JP S5925927 AManufacture of steel pipe—3
JP S6210241 ASteel for seamless drawn oil well pipe excellent in corrosion resistance and collapsing strength—5
JP S6210240 ASteel for seamless drawn oil well pipe excellent in corrosion resistance and collapsing strength—7
JP H05255794 AHeat resistant magnesium alloy—5
WO 9,325,799 A1Method of creating a wellbore in an underground formation—75
JP H07507610 A地層中に坑井を設ける方法—9
EP 0,733,715 A2Hot-rolled steel sheet and method for forming hot-rolled steel sheet having low yield ratio, high strength and excellent toughness—24
JP H09287027 AProduction of high strength, high toughness and seamless steel pipe—12
WO 9,800,626 A1Method for expanding a steel tubing and well with such a tubing—109
JP H10176239 AHigh strength and low yield ratio hot rolled steel sheet for pipe and its production—46
US 5,993,570 ALinepipe and structural steel produced by high speed continuous casting199946
US 6,331,216 B1Steel pipe having high ductility and high strength and process for production thereof200125
JP 2002129283 ASteel pipe having excellent expanding workability—19
JP 2002266055 AOil well steel pipe for expansion—11
JP 2002349177 ASteel pipe for burying and expansion and burying method of oil well steel pipe—9
US 2003145920 A1High tensile strength cold rolled steel sheet having excellent strain age hardening characteristics and the production thereof—18
WO 2004/001076 A1Oil well steel pipe excellent in crushing resistance characteristics after pipe expansion—9
US 2004035576 A1Steel pipe for embedding-expanding, and method of embedding-expanding oil well steel pipe—8
WO 2004/031420 A1High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method—27
US 6,723,453 B2Welded steel pipe having excellent hydroformability and method for making the same20042
JP 2005146414 AExpansive seamless steel pipe for use in oil well and method for production thereof—17
WO 2005/080621 A1Steel sheet or steel pipe being reduced in expression of baushinger effect, and method for production thereof—17
US 2005217768 A1Oil country tubular goods excellent in collapse characteristics after expansion and method of production thereof—25
JP 2006009078 ASeamless steel pipe for oil well use having excellent expandability—17
EP 1,717,331 A1Steel sheet or steel pipe being reduced in expression of baushinger effect, and method for production thereof—3
US 2007116975 A1Seamless expandable oil country tubular goods and manufacturing method thereof—11
US 2007199720 A1Steel pipe for embedding-expanding, and method of embedding-expanding oil well steel pipe—2

Non-Patent Literature (1)

  • Material Properties, Formability Testing of Sheet Metals, Metalworking: Sheet Forming, vol. 14B, ASM Handbook, ASM International, 2006, pp. 673-696. http://products.asminternational.org.