Abstract

The present invention provides a method for upgrading low-rank coal unsuitable for production of a reduced metal by a conventional carbon composite method to produce an upgraded coal suitable for the carbon composite method. The prevent invention also provides a method for producing a high-quality reduced metal using the upgraded coal as a carbonaceous material to be incorporated. In these methods, coal is first aged by heating in an organic solvent to produce upgraded coal for metallurgy having higher thermal plasticity than that of the coal. Then, a mixture of the upgraded coal for metallurgy and a metal oxide-containing raw material is agglomerated by an agglomerator, and the resultant agglomerates are reduced by heating in a moving hearth furnace and then melted by further heating to produce a reduced melt. The reduced melt is cooled and solidified in the moving hearth furnace to produce a reduced solid, and then the reduced solid is discharged to the outside of the furnace. Then, a slag is removed using a screen to recover a metal as a reduced metal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing upgraded coal for metallurgy comprising: mixing a low rank coal and an organic solvent in a slurry preparation tank to prepare a raw material slurry; aging the raw material slurry in an aging tank by heating to extract a soluble component of the low rank coal in the organic solvent to prepare an extracted slurry; and removing the organic solvent from the extracted slurry by evaporation to produce upgraded coal for metallurgy as a solid form; wherein hydrogen is not added to the slurry preparation tank or the aging tank and the organic solvent is not rehydrogenated.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the solvent removal comprises: sedimenting an insoluble component of the coal by allowing the extracted slurry to stand to separate between a supernatant containing an extracted coal, which is the extracted soluble component,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • T. Yoshida, et al., "The Effect of Extraction Condition on ‘Hypercoal’ Production (1)-Under Room-Temperature Filtration", Fuel, XP 004354921, vol. 81, No. 11-12, Jul. 8, 2002, pp. 1463-1469.
  • T. Yoshida, et al., "The Effect of Extraction Condition on 'Hypercoal' Production (1)-Under Room-Temperature Filtration", Fuel, XP 004354921, vol. 81, No. 11-12, Jul. 8, 2002, pp. 1463-1469.
  • U.S. Appl. No. 12/442,966, filed Mar. 26, 2009, Okuyama, et al.