Patents
US 7,790,799 B2#131659700 Most CitedActiveUnited States (USPTO)Utility

Reinforced silica/elastomer composite

0Forward Citations (#131659700 Global)
0.0/yrCitation Velocity (#131659700 Global)
0.56Citation PageRank (#131659700 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

This invention is based upon the discovery that elongated silica has superior characteristics for reinforcing rubbery elastomers as compared to conventional silica. More specifically, elongated silica provides a higher level of reinforcement for elastomers at the same level of loading. Accordingly, elongated silica can be employed to attain an equivalent level of reinforcement at a lower level of loading. This results in lower weight compositions and potential cost savings. Rubber compounds that are reinforced with elongated silica offer significant advantages in tires including reduced rolling resistance, increased tread life, and, of course, reduced weight. The subject invention more specifically relates to a tire having a tread wherein said tread is comprised of a silica reinforced rubber composition, wherein the silica reinforced rubber composition is comprised of (1) a rubbery polymer and (2) an elongated silica, wherein the elongated silica has a width that is within the range of about 5 nm to about 40 nm, and wherein the elongated silica has a length of about 40 nm to about 300 nm. The present invention also discloses a process for preparing a silica reinforced rubber compos

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a silica reinforced rubber composition which comprises (1) adding an elongated silica to a latex of a rubbery polymer, wherein the elongated silica has a width that is within the range of about 5 nm to about 40 nm, and wherein the elongated silica has a length of about 40 nm to about 300 nm, and (2) recovering the silica reinforced rubber composition from the latex.

  2. Claim 2Depends on #1

    A process as specified in claim 1 wherein the elongated silica is added in an amount which is within the range of about 20 phr to about 70 phr.

  3. Claim 3Depends on #1

    A process as specified in claim 1 wherein the elongated silica is added in an amount which is within the range of about 30 phr to about 60 phr.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.