Method to increase the compressive stress of PECVD dielectric films
Abstract
A method for forming a compressive stress carbon-doped silicon nitride layer is provided. The method includes forming an initiation layer and a bulk layer thereon, wherein the bulk layer has a compressive stress of between about −0.1 GPa and about −10 GPa. The initiation layer is deposited from a gas mixture that includes a silicon and carbon-containing precursor and optionally a nitrogen and/or source but does not include hydrogen gas. The bulk layer is deposited from a gas mixture that includes a silicon and carbon-containing precursor, a nitrogen source, and hydrogen gas. The initiation layer is a thin layer that allows good transfer of the compressive stress of the bulk layer therethrough to an underlying layer, such as a channel of a transistor.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 8.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of depositing a two layer film having compressive stress, comprising: depositing an initiation layer comprising silicon and carbon on a substrate in a chamber from a first gas mixture in the presence of a low frequency RF power, wherein the first gas mixture comprises a silicon and carbon-containing precursor; and then turning on a high frequency RF power and depositing a bulk layer comprising silicon, carbon, and nitrogen on the initiation layer from a second gas mixture in the presence of the high frequency RF power, wherein the second gas mixture comprises the silicon and carbon-co
- Claim 2Depends on #1
The method of claim 1 , wherein the silicon and carbon-containing precursor is selected from the group consisting of alkylsilane
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (5)
- First Office Action dated Jun. 26, 2009, issued by the State Intellectual Property Office of the People's Republic of China in Chinese Patent Application Serial No. 200710165143.8.
- Notice to File a Response dated Sep. 11, 2009, issued by the Korean Intellectual Property Office in KR 1020070103998.
- U.S. Appl. No. 11/245,373, filed Oct. 6, 2005, Entitled: Method and Apparatus for the low Temperature Deposition of Doped Silicon Nitride Films.
- U.S. Appl. No. 11/478,273, filed Jun. 29, 2006, Entitled: Decreasing the Etch Rate of Silicon Nitride by Carbon Addition.
- U.S. Appl. No. 60/805,324, filed Jun. 20, 2006, Entitled: Method to Increase Silicon Nitride Tensile Stress Using Nitrogen Plasma In-Situ Treatment and Ex-Situ UV Cure.