US 7,785,941 B2#28069012 Most CitedActiveUnited States (USPTO)Utility

Method of fabricating thin film transistor

3Forward Citations (#28069012 Global)
0.2/yrCitation Velocity (#34640755 Global)
1.68Citation PageRank (#19229960 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for fabricating a thin film transistor (TFT) is provided. A substrate having a gate, a dielectric layer, a channel layer and an ohmic contact layer formed thereon is provided. Next, a metal layer is formed over the substrate covering the ohmic contact layer. Next, the metal layer and the ohmic contact layer are simultaneously etched by a wet etching process to form a source/drain and expose the channel layer. Because the wet etching process can be used to selectively etch the ohmic contact layer, damage to the underlying channel layer may be negligible. Thus, the reliability of the device may be promoted. Furthermore, the process may be simplified, the production yield and the throughput of TFT may be increased.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a source/drain of a thin film transistor (TFT), comprising: providing a substrate comprising a gate, a dielectric layer, a channel layer and an ohmic contact layer formed thereon; forming a metal layer over the substrate to cover the ohmic contact layer; and etching the metal layer and the ohmic contact layer simultaneously by using a wet etching process to form a source/drain and expose the channel layer, wherein an etchant used in said wet etching process comprises an aqueous solution of mixture of hydrogen peroxide, phosphoric acid and hydrofluoric acid.

  2. Claim 2Depends on #1

    The method as claimed in claim 1 , wherein a concentration of hydrogen peroxide in said etchant is in a range of 3˜30 wt. %.

  3. Claim 3Depends on #1

    The method as claimed in claim 1 , wherein a concentration of phosphoric acid in said etchant is in a range of 0.1˜10 wt. %. 4

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗