Abstract

The present invention relates to methods for improving deposited film uniformity and controlling the erosion of sputter targets. Improved methods for achieving predetermined microstructure orientation in copper hollow cathode magnetron (HCM) sputter targets and targets prepared by such methods are disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a hollow cathode magnetron sputter target comprising the steps of: providing a copper billet; hot forging the billet by heating the billet for about 75 minutes at a temperature of from about 1650° F. to about 1750° F.; upset forging the billet to a predetermined first dimension to achieve a part; rotating the part by first, second and third successive 90° increments and alternating rotary forging and upset forging to a successive predetermined dimension; quenching the part; heating the part for about 75 minutes at about 1112° F.+/−50° F.; upset forging the part to a predet

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Clark et al., "Influence of Initial Ingot Breakdown on the Microstructural and Textural Evelopment of High-Purity Tantalum", Metallurgical Transactions A:Physical Metallurgy and Materials Sxience, vol. 22A (12), Dec. 1991, pp. 2959-2968.
  • Hojas, "Radial Forging," Metals Handbook, 9.sup.th Edition, vol. 14, p. 145-149. (1988).