Patents
US 7,776,162 B2#29436744 Most CitedExpiredUnited States (USPTO)Utility

Steels with few alumina clusters

3Forward Citations (#29436744 Global)
0.2/yrCitation Velocity (#34795381 Global)
1.31Citation PageRank (#28169848 Global)
23Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A steel having few alumina clusters prepared by casting liquid steel deoxidized with Al, with the addition of one or more rare-earth metals (REM) selected from the group of Ce, La, Pr and Nd in which: (a) The REM-oxide-content in oxide-based inclusions consisting mainly of alumina and REM-oxides is 0.5 to 15 mass % of said oxide-based inclusions, or (b) The mass ratio of total REM to total oxygen (T.O.), REM/T.O., in liquid steel is not less than 0.05 and not more than 0.5, in addition to (a), or (c) The total REM-content is not less than 0.1 ppm and less than 10 ppm and the dissolved-REM-content is less than 1 ppm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A steel prepared by casting liquid steel deoxidized with Al, including one or more rare-earth metals (REMs) selected from the group of Ce, La, Pr and Nd, characterized by, the steel containing alumina clusters and consisting essentially of C of 0.0005 to 1.5 mass %, Si of 0.005 to 1.2 mass %, Mn of 0.05 to 3.0 mass %, P of 0.001 to 0.1 mass %, S of 0.0001 to 0.05 mass %, Al of 0.005 to 1.5 mass %, and total oxygen T.O. of less than 80 ppm, with the remainder iron and unavoidable impurities, where the alumina clusters are oxide-based inclusions consisting essentially of alumina and REM-oxide, t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 2,980,529 AMethod of making aluminum killed steel196113
US 3,623,862 AUse of rare earth elements for reducing nozzle deposits in the continuous casting of steel process197113
JP S5270918 APreparation of clean steel of lonon-metallic inclusion—7
US 4,042,381 AControl of inclusion morphology in steel19778
JP S565915 AProduction of steel for steel cord—6
JP S5647510 AProduction of very fine wire material having good extension property—6
US 4,440,568 ABoron alloying additive for continuously casting boron steel198415
US 4,880,480 AHigh strength hot rolled steel sheet for wheel rims19898
JP H0770638 AProduction of steel pipe and stock for column excellent in long time high temperature strength and toughness—1
JP H09192799 AMethod for preventing clogging of immersion nozzle in continuous casting—6
EP 0,829,546 A1Process for producing aluminum-killed steel free of cluster—18
JP H10183229 AProduction of high carbon steel wire rod—17
EP 0,906,960 A1Titanium killed steel sheet and method—16
JP H11264048 AHigh-strength steel plate excellent in toughness of welded zone—9
JP H11323426 AProduction of high clean steel—11
JP 2000144330 ASlab for thin steel sheet small in defect caused by inclusion and its production—8
EP 1,029,938 A2Rolled steel having few inclusion defects—6
US 6,120,578 AMethod of producing cluster-free Al-killed steel200020
JP 2000273524 AProduction of high cleanliness steel—2
JP 2001026842 ACold rolled steel sheet excellent in surface property and internal property and its production—15
US 6,221,180 B1Steel sheet for can and manufacturing method thereof200116
US 6,344,093 B1High tensile strength steel product for high heat input welding, having excellent toughness in heat-affected zone200214
JP 2002105527 AMethod for producing high cleanliness steel—6

Non-Patent Literature (4)

  • "Rapid Evaluation of Inclusion in Steel with the use of Cold crucible" CAMP-ISIJ, vol. 14 (2001), p. 817-819.
  • H. Yin et al. ""In-situ" Observation of Collision, Agglomeration and Cluster Formation of Alumina Inclusion Particles on Steel Melts", ISIJ International, vol. 37 (1997), No. 10, p. 936-945.
  • Shirota et al. "Development of Production Process of Highly Clean Steel" CAMP-ISIJ, vol. 4 (1991), p. 1214-1217.
  • Yasunaka et al. "Pinhole and Inclusion Defects Formed at the Subsurface in Ultra Low carbon Steel" The Iron and Steel Institute of Japan, vol. 81 (1995), No. 5 p. 17-22.