Patents
US 7,767,783 B2#148870179 Most CitedActiveUnited States (USPTO)Utility

Poly (arylene sulfide) and production process thereof

0Forward Citations (#148870179 Global)
0.0/yrCitation Velocity (#148870179 Global)
0.56Citation PageRank (#148870179 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A dehydration step is conducted by heating a mixture containing an organic amide solvent and a sulfur source including an alkali metal hydrosulfide, and a part of an overall charged amount of an alkali metal hydroxide as needed. The mixture remaining within the system after the dehydration step is mixed with a dihalo-aromatic compound, the resultant mixture is heated to conduct a polymerization reaction, and the alkali metal hydroxide is added to the mixture for polymerization reaction continuously or in portions to control the pH of the mixture for polymerization reaction within a range of from 7 to 12.5 from the beginning to the end of the polymerization reaction. The poly(arylene sulfide) according to the present invention has a nitrogen content of at most 800 ppm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A poly(arylene sulfide) obtained by polymerization of a sulfur source and a dihalo-aromatic compound in the presence of an alkali metal hydroxide in an organic amide solvent, the polymerization medium having a pH in a range of from 7 to 12.5 from the beginning to the end of the polymerization reaction, the poly(arylene sulfide) having a nitrogen content of at most 800 ppm.

  2. Claim 2Depends on #1

    The poly(arylene sulfide) according to claim 1 , wherein the nitrogen content is at most 600 ppm.

  3. Claim 3Depends on #1

    The poly(arylene sulfide) according to claim 1 , wherein the melt viscosity thereof is 10 to 1,500 Pa·s as measured at a temperature of 310° C. and a shear rate of 1,216 sec −1 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
JP S617332 AProduction of high molecular weight polyarylene sulfide—60
US 4,645,826 AProcess for production of high to ultra-high molecular weight linear polyarylenesulfides1987125
JP S6243422 AProduction of polyarylene sulfide—5
EP 0,215,312 A1Method for producing of polyarylene sulfides—21
JP S6346228 AProduction of polyarylene sulfide having excellent handling property—12
EP 0,259,984 A1Process for producing a polyarylene sulfide—22
US 4,767,841 AArylene sulfide polymer preparation from dehydrated admixture comprising sulfur source, cyclic amide solvent and water198844
JP S63243134 AProduction of polyarylene sulfide—7
US 4,786,711 AP-phenylene sulfide polymer preparation with dehydrated mixture of alkali metal hydroxide and excess alkali metal bisulfide198838
JP S63289025 AImproved manufacture of poly(p-phenylenesulfide)—7
US 4,794,164 AProcess for producing a polyarylene sulfide of excellent handling property and a polyarylene sulfide produced by the process thereof198852
US 4,810,773 AMethod for producing polyarylene sulfide with lithium halide catalyst198914
JP H01245030 ABiaxially oriented poly-p-phenylene sulfide film—11
JP H02160834 AProduction of polyarylene sulfide—10
JP H02302436 AProduction of polyarylene sulfide—16
JP H05271414 AProduction of high-molecular-weight polyarylene sulfide—12
JP H09286861 AProduction of polyarylene sulfide—38
US 5,840,830 AProcess for producing poly(arylene sulfide)199847
JP 2001040090 APolyarylene sulfide, its production and polyarylene sulfide composition—24
JP 2001181394 AMethod of manufacturing polyarylene sulfide—32