Patents
US 7,767,589 B2#8643967 Most CitedActiveUnited States (USPTO)Utility

Passivation layer for a circuit device and method of manufacture

12Forward Citations (#8643967 Global)
0.8/yrCitation Velocity (#9961190 Global)
1.81Citation PageRank (#17083272 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

According to one embodiment of the disclosure, a method for passivating a circuit device generally includes providing a substrate having a substrate surface, forming an electrical component on the substrate surface, and coating the substrate surface and the electrical component with a first protective dielectric layer. The first protective dielectric layer is made of a generally moisture insoluble material having a moisture permeability less than 0.01 gram/meter2/day, a moisture absorption less than 0.04 percent, a dielectric constant less than 10, a dielectric loss less than 0.005, a breakdown voltage strength greater than 8 million volts/centimeter, a sheet resistivity greater than 1015 ohm-centimeter, and a defect density less than 0.5/centimeter2.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an integrated circuit comprising: providing a substrate having a substrate surface; forming an electrical component comprising at least a transistor or a capacitor on the substrate surface; coating the substrate surface and electrical component with a first protective dielectric layer made of alumina, the first protective dielectric layer having a thickness that is in the range of approximately 50 to 2000 angstroms; etching a portion of the first protective dielectric layer from the substrate surface or the electrical component in order to form a contact surface; for

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,890,636 AMultilayer wiring structure of integrated circuit and method of producing the same197585
JP H02307247 AMultilayer interconnection—12
US 5,548,099 AMethod for making an electronics module having air bridge protection without large area ablation199667
DE 19,719,179 A1Semiconductor module, e.g. LSI circuit, with air bridge wiring—8
US 5,949,144 APre-bond cavity air bridge199938
US 6,489,233 B2Non-metallic barrier formations for copper damascene type interconnects200228
US 2003141096 A1Metallic coated dielectric substrates—44
US 6,607,934 B2Micro-electromechanical process for fabrication of integrated multi-frequency communication passive components200353
WO 2005/020343 A1Method for sealing thin film transistors—16
US 6,956,283 B1Encapsulants for protecting MEMS devices during post-packaging release etch2005162
EP 1,732,149 A1Barrier layer for an organic electronic device—9
US 2007054127 A1Silane coating compositions, coating systems, and methods—29
US 7,344,972 B2Photosensitive dielectric layer200816
US 2008185173 A1Environmental Protection Coating System and Method—40
US 2008185174 A1Passivation Layer for a Circuit Device and Method of Manufacture—25
US 2009134401 A1Thin Film Transistor and Display Device, Method for Manufacturing the Same, and Television System—26
US 2009191665 A1Electronic Device and Method of Manufacturing Same—35
US 2009290314 A1Environmental Protection Coating System and Method—17
US 2009291200 A1Environmental Protection Coating System and Method—29

Non-Patent Literature (5)

  • Bedinger et al., "Environmental Protection Coating System and Method," U.S. App. No. 11/848,891, 57 pages, 9 pages of drawings, filed Aug. 31, 2007.
  • Bedinger et al., "Environmental Protection Coating System and Method," U.S. App. No. 12/533,409, 40 pages, 9 pages of drawings, filed Jul. 31, 2009.
  • Bedinger et al., "Environmental Protection Coating System and Method," U.S. App. No. 12/533,448, 36 pages, 9 pages of drawings, filed Jul. 31, 2009.
  • Bedinger et al., "Environmental Protection Coating System and Method," U.S. App. No. 12/533,503, 45 pages, 9 pages of drawings, filed Jul 31, 2009.
  • Bedinger, "Response to Election Restriction Requirement," electronically filed with the USPTO on Jun. 19, 2009, 2 pages.