hottubpatentshottub.tech
US 7,767,548 B2#174861 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing semiconductor wafer including a strained silicon layer

0Forward Citations (#174861 Global)
0.0/yrCitation Velocity (#174861 Global)
0.98Citation PageRank (#174861 Global)
2Prior Art Cited
14Structured Claims
0Drawings / Sheets

Abstract

A method for manufacturing a semiconductor wafer with a strained Si layer having sufficient tensile strain and few crystal defects, while achieving a relatively simple layered structure, is provided. The method includes the steps of: (a) forming an SiGe mixed crystal layer 12 and a first Si layer 13 in this order on the surface of a silicon wafer 11 ; (b) forming an SiO 2 layer 16 on top of the first Si layer and/or a support wafer 14 ; (c) forming a layered product 17 by stacking the silicon wafer and the support wafer with the SiO 2 layer being placed therebetween; (d) forming a second Si layer 18 by thinning the silicon wafer of the layered product; (e) implanting hydrogen ion and/or rare gas ion, such that ionic concentration peaks in a predetermined area; (f) subjecting the layered product to a first heat treatment; and (g) carrying out a second heat treatment following the first heat treatment, thereby relaxing the SiGe mixed crystal layer and diffusing Ge through portions of the first Si layer and the second Si layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.

Claims (14)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor wafer, comprising: (a) forming a SiGe mixed crystal layer and a first Si layer in this order on a surface of a silicon wafer; (b) forming a SiO 2 layer on top of the first Si layer, on a separately prepared support wafer which is prepared separately from the first Si layer, or on the first Si layer and the support wafer; (c) forming a layered product by stacking the silicon wafer and the support wafer with the SiO 2 layer being placed therebetween; (d) forming a second Si layer by thinning the silicon wafer of the layered product to a predetermined thickness; (e) implanting hydrogen ions, rare gas ions, or both hydrogen ions and rare gas ions, to form ionic concentration peaks in an area which includes an interface between the first Si layer and the SiO 2 layer, and also includes the first Si layer from the interface up to one half a thickness thereof; (f) carrying out a first heat treatment by maintaining the layered product in an inert gas atmosphere containing nitrogen or Argon gas at 450 to 600° C. for 15 to 600 minutes; and (g) carrying out a second heat treatment following the first heat treatment, by maintaining the layered product at 800 to 1000° C. for 15 to 300 minutes, thereby relaxing the SiGe mixed crystal layer and diffusing Ge through portions of the first Si layer and the second Si layer.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising (h) carrying out a third heat treatment, following the second heat treatment, by maintaining the layered product in an oxidizing atmosphere at 1100 to 1300° C. for 1 to 600 minutes.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the support wafer is an insulating substrate selected from the group consisting of quartz, sapphire, SiC, and aluminum nitride.

  4. Claim 4Depends on #1

    The method of claim 1 , wherein the amount of Ge in the mixed crystal layer to be formed is from 3 to 30%.

  5. Claim 5Depends on #1

    The method of claim 1 , wherein the SiGe mixed crystal layer is formed to a thickness of 20 nm to 1 μm.

  6. Claim 6Depends on #1

    The method of claim 1 , wherein the first Si layer is formed to a thickness of 5 to 50 nm.

  7. Claim 7Depends on #1

    The method of claim 1 , wherein the SiO 2 layer is formed to a thickness of 50 to 1000 nm.

  8. Claim 8Depends on #1

    The method of claim 1 , wherein the second Si layer is thinned to a thickness of preferably 30 to 300 nm.

  9. Claim 9Depends on #1

    The method of claim 1 , wherein the thinning is carried out by grinding, polishing, wet etching with an acid or alkali solution, vapor-phase etching with plasma, or lapping.

  10. Claim 10Depends on #1

    The method of claim 1 wherein the heat treatment is carried out by maintaining the layered product in an argon gas atmosphere at 1100° C. for 120 minutes.

  11. Claim 11Depends on #1

    The method of claim 1 , wherein the hydrogen ions, rare earth ions, or both are implanted within half the thickness of the first Si layer from the interface between the first Si layer and the SiO 2 layer.

  12. Claim 12Depends on #1

    The method of claim 1 , wherein the rare earth ions are selected from the group consisting of helium ions and neon ions.

  13. Claim 13Depends on #1

    The method of claim 1 , wherein the area of (e) also includes the first Si layer from the interface up to one fourth a thickness thereof.

  14. Claim 14Independent Claim

    A method for manufacturing a semiconductor wafer, comprising: (A) forming a SiGe mixed crystal layer and a first Si layer in this order on a surface of a silicon wafer; (B) forming an SiO 2 layer on top of the first Si layer, a support wafer which is prepared separately from the first Si layer, or on both the first Si layer and the support wafer; (C) forming a damaged layer at an ion implantation position within the silicon wafer by implanting hydrogen or rare gas ions, to form ionic concentration peaks at 0.3 to 1.0 μm below a surface of the first Si layer within the silicon wafer; (D) forming a layered product by stacking the silicon wafer and the support wafer ( 24 ) with

Technical Overview & Description

BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method for manufacturing a semiconductor wafer having formed on its surface a strained Si layer with internal two-dimensional tensile strain. 2. Description of the Related Art As used herein, Patent Document 1 refers to Japanese Laid-Open Patent Publication No. 9-180999 (claim 2 and paragraphs [0020], [0021] and [0031]) and Patent Document 2 Japanese Laid-Open Patent Publication No. 11-233440 (claim 2 and paragraph [0006]) Reportedly, in order to enhance the performance of semiconductor devices employing a silicon single crystal, it is effective to increase the mobility of electrons or holes in the silicon single crystal. Specifically, the mobility of carriers is enhanced by employing a strained Si layer with internal two-dimensional tensile strain as a silicon layer where the electrons or holes flow, and therefore, based on this technique, for example, C-MOS devices capable of operating at high speed have been studied. A semiconductor wafer with a strained Si layer is manufactured by forming a relaxed SiGe layer, which has a larger lattice constant than Si, on an Si wafer through epitaxy, and forming the strained Si layer through epitaxial growth of a thin Si layer on the relaxed SiGe layer. Since the SiGe layer formed on the Si wafer has a Ge concentration of up to 30%, crystal defects such as misfit dislocation occur due to the difference in lattice constant between the Si substrate and the SiGe layer, adversely affecting the strained Si layer formed on the SiGe layer. The density of crystal defects caused by conventional manufacturing methods is in the range of approximately 1×10 5 to 1×10 7 defects/cm 2 . To solve this problem, some methods have been proposed, including a method employing a buffer layer with a composition ratio of Ge in SiGe being increased at a constant gentle gradient, a method employing a buffer layer with a stepwise cha

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (2)

PatentTitleYearCitations

Non-Patent Literature (2)

  • English Abstract of Japanese Patent Publication No. JPH 09-180999, published Jul. 11, 1997.
  • English Abstract of Japanese Patent Publication No. JPH 11-233440, published Aug. 27, 1999.