Material and method of manufacture of a solder joint with high thermal conductivity and high electrical conductivity
Abstract
The present invention provides a powder blend or composite powder that is fed into a kinetic spray device, accelerated towards a substrate or part in order to form a composite solder with thermal and electrical properties better than existing solder. The other advantages of building a solder layer in this manner include a low oxide content to improve subsequent solderability, excellent control of the deposition thickness, excellent control of the deposition chemistry and lastly, high speed of manufacture.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming a composite solder coating on a substrate comprising the steps of: providing powder materials comprising a solid metal matrix material and a filler material, wherein said solid metal matrix material is one or more of tin-silver-copper (Sn—Ag—Cu), tin-copper (Sn—Cu), tin-copper-nickel (Sn—Cu—Ni), tin-silver (Sn—Ag), tin-silver-bismuth (Sn—Ag—Bi), tin-bismuth-indium (Sn—Bi—In), tin-gold (Au—Sn), tin-zinc (Sn—Zn), tin-zinc-bismuth (Sn—Zn—Bi), tin-bismuth-silver (Sn—Bi—Ag), tin (Sn), tin-indium (Sn—In), indium (In), indium-silver (In—Ag), and tin-lead (Sn—Pb), and wherein said
Technical Overview & Description