Patents
US 7,753,989 B2#30361654 Most CitedActiveUnited States (USPTO)Utility

Direct passivation of metal powder

3Forward Citations (#30361654 Global)
0.2/yrCitation Velocity (#34845799 Global)
1.22Citation PageRank (#31113248 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of producing passivated Ti or Ti alloy particles with oxygen concentrations of less than about 900 parts per million (ppm), which includes introducing a halide vapor of Ti or the metal constituents of the alloy at sonic velocity or greater into a stream of liquid alkali or liquid alkaline earth metal or mixtures thereof forming a reaction zone in which the halide is reduced by the liquid metal present in sufficient excess of stoichiometric such that Ti or Ti alloy powder from the reduction of the halide by the liquid metal is friable. After filtration and distillation excess liquid metal is removed from the Ti or Ti alloy powder that is then maintained at elevated temperature for a time sufficient to grow the particles to average diameters calculated from BET surface area measurement greater than about one micron. After cooling the Ti or Ti alloy powder to temperature of about 80° C. or less, the cooled Ti or Ti alloy powder is contacted with air and/or water to passivate the particles to produce friable metal powder and to remove other reaction products. A system for accomplishing the method is also shown.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a friable, passivated metal powder, comprising the steps of: introducing a metal halide vapor into a stream of liquid metal present in stoichiometric excess, wherein the stream of liquid metal is selected from the group consisting of alkali metals, alkaline earth metals, or mixtures thereof, to thereby form a reaction zone in which the metal halide vapor is reduced by the liquid metal to form reaction products; separating substantially all of the excess liquid metal from the reaction products, wherein the reaction products include a metal powder; growing the metal powder

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 1,771,928 AFilter press193063
US 2,205,854 AMethod for manufacturing titanium and alloys thereof1940193
US 2,607,675 ADistillation of metals195244
US 2,647,826 ATitanium smelting process195366
GB 722,184 AImprovements in or relating to the production of pure titanium and zirconium—8
GB 778,021 AProcess for the production of titanium—7
US 2,816,828 AMethod of producing refractory metals195738
US 2,823,991 AProcess for the manufacture of titanium metal195850
US 2,827,371 AMethod of producing titanium in an agitated solids bed195841
US 2,835,567 AMethod of producing granular refractory metal195821
US 2,846,304 AMethod of producing titanium195828
US 2,846,303 AMethod of producing titanium195835
US 2,882,143 AContinuous process for the production of titanium metal195939
US 2,882,144 AMethod of producing titanium195925
US 2,890,112 AMethod of producing titanium metal195938
US 2,895,823 AMethod of further reducing the reaction products of a titanium tetrachloride reduction reaction195925
US 2,915,382 AProduction of metals195913
US 2,941,867 AReduction of metal halides196042
US 2,944,888 AManufacture of titanium196026
US 3,058,820 AMethod of producing titanium metal196214
US 3,067,025 AContinuous production of titanium sponge196285
US 3,085,871 AMethod for producing the refractory metals hafnium, titanium, vanadium, silicon, zirconium, thorium, columbium, and chromium196329
US 3,085,872 AMethod for producing the refractory metals hafnium, titanium, vanadium, silicon, zirconium, thorium, columbium, and chromium196326
US 3,113,017 AMethod for reacting titanic chloride with an alkali metal196313
US 3,331,666 AOne-step method of converting uranium hexafluoride to uranium compounds196727
US 3,519,258 ADevice for reducing chlorides197030
US 3,535,109 AMethod for producing titanium and other reactive metals197018