Anti-glare film, method for manufacturing the same, and display device using the same
Abstract
An anti-glare film has a plurality of diffuser elements, and has specified optical properties. The ratio of I(α+1)/I(α) is more than 0.1 to 0.6, where I(α) is an intensity of a light reflected toward an arbitrary angle α of 10° or less from a specular reflection direction of an incident light upon the surface at an angle of 5° to 30° from the surface normal, and I(α+1) is an intensity of a reflected light deviated from the arbitrary angle α by 1° in a wide-angle direction. The gain of a light reflected in the direction at 20° or more from the specular reflection direction of the incident light is 0.02 or less, in which the gain is obtained by normalizing a reflected light intensity using a specular reflection intensity of a standard diffuse plate as 1. The diffuser elements have an average space therebetween of 50 to 300 micrometers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An anti-glare film, comprising: a substrate; and an anti-glare layer formed on the substrate, wherein the anti-glare layer has diffuser elements thereon, the diffuser elements on the anti-glare layer are formed by applying a coating composition including organic fine particles on the substrate and causing convection in the coating composition so that the fine particles are agglomerated in the in-plane direction, the fine particles have an average particle diameter ranging from 4 μm to 15 μm, the anti-glare layer has a dried film thickness ranging from 4 μm to 15 μm, and the fine particles are
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗