Polymer solution for nanoimprint lithography to reduce imprint temperature and pressure
Abstract
A method of forming features on substrates by imprinting is provided. The method comprises: (a) forming a polymer solution comprising at least one polymer dissolved in at least one polymerizable monomer; and (b) depositing the polymer solution on a substrate to form a liquid film thereon; and then either: (c) curing the liquid film by causing the monomer(s) to polymerize and optionally cross-linking the polymer(s) to thereby form a polymer film, the polymer film having a glass transition temperature (T g ); and imprinting the polymer film with a mold having a desired pattern to form a corresponding negative pattern in the polymer film, or (d) imprinting the liquid film with the mold and curing it to form the polymer film. The temperature of imprinting is as little as 10° C. above the T g , or even less if the film is in the liquid state. The pressure of the imprinting can be within the range of 100 to 500 psi.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An imprintable polymer solution for imprinting, said polymer solution comprising: at least one polymer dissolved in at least one polymerizable monomer; at least one component selected from the group consisting of at least one cross-linker and at least one viscosity modifier; and at least one photoinitiator selected from the group consisting of α-hydroxy-ketones, α-amino-ketones, and benzophenones; wherein said at least one cross-linker is selected from molecules that have difunctional polymerizable groups, and wherein said at least one cross-linker is selected from the group consisting of ethy
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (5)
- Chou et al., Science vol. 272 (Apr. 5, 1996).
- Chou, et al., "Imprint Lithography with 25-Nanometer Resolution," Science, vol. 272, Apr. 5, 1996, pp. 85-87.
- Khang, et al., "Room-temperature Imprint Lithography by Solvent Vapor Treatment," Applied Physics Letters, vol. 76, No. 7, Feb. 14, 2000, pp. 870-872.
- Lebib, A et al-"Room-Temperature and Low-Pressure Nanoimprint Lithography"-Jul. 2002-pp. 61-62.
- Matsui, et al., "Room Temperature Replication in Spin on Glass by Nanoimprint Technology," Journal of Vacuum Science Technology B, vol. 19, No. 6, Nov./Dec. 2001, pp. 2801-2805.