High purity magnetite formation process and apparatus, and product thereof

3Forward Citations (#32900927 Global)
0.2/yrCitation Velocity (#34935833 Global)
1.07Citation PageRank (#37795007 Global)
20Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process of producing magnetite with a high purity of greater than 90% magnetite, more typically greater than 98% magnetite, by reducing powdered hematite into magnetite under maximum temperatures of about 700 to 1300° C. against a counter-current of or concurrent with methane or natural gas in a heating device. The amount of methane used to reduce the hematite may be about 0.18 and 1.8 standard cubic feet of methane per pound of hematite. A product of high purity methane produced from the process is also provided, where the magnetite is below 1 μM in diameter and has a magnetic saturation greater than 90.0 emu/g. Corresponding apparatus using an improved feeder system for powdered hematite is provided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing high purity magnetite comprising the steps of: feeding hematite into a feed zone of a heating device for movement therethrough, the heating device further having a discharge zone, feeding gas into the heating device for movement therethrough, and heating a portion of the heating device to a maximum temperature in a range of about 700 to 1300° C., to convert said hematite into said high purity magnetite, and cooling the high purity magnetite in an atmosphere selected from the group consisting of a reducing gas atmosphere and an oxygen-free atmosphere, prior to the high p

  2. Claim 2Depends on #1

    The process of claim 1 , including employing a maximum temperature in a range of about 750 to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 672,192 AManufacture of material for filtering.19018
US 2,545,932 ATwo-stage conversion of iron oxide into iron195111
US 2,693,409 ATreatment of iron ore195433
US 2,694,656 AMagnetic impulse record member, magnetic material, and method of making magnetic material195442
US 2,900,236 AProduction of ferromagnetic iron oxide195924
US 3,210,180 ATemperature control of iron ore reducing fluidized beds196514
US 3,276,858 AMethod for carrying out gas-solids reactions196610
US 3,843,773 AProcess for producing fine acicular gamma ferric oxide crystals197423
US 3,928,709 AFerrous ferric oxides, process for preparing same and their use in magnetic recording197534
US 4,311,684 AProcess for producing iron oxide containing magnetite198217
US 4,376,714 AProcess for preparing acicular iron oxide particles198326
US 4,436,681 AProcess for producing iron oxide weighting material from iron chloride solutions198428
US 4,629,500 AUse of novel rotary tubular kiln198616
US 4,822,509 AHighly magnetic iron oxide powder198913
US 5,348,160 ACoal cleaning process199422
US 5,512,195 AProcess for producing single phase magnetite powder19968
US 5,794,791 ACoal cleaning process199890
US 5,837,051 AProcess for the thermal treatment of iron oxides in a circulating fluidized bed199810
US 6,302,952 B1Process for the production of black iron oxide pigments200122
US 6,827,757 B2Magnetite-iron based composite powder, magnetite-iron based powder mixture, method for producing the same, method for remedying polluted soil, water or gases and electromagnetic wave absorber200424