Rinsing fluid for lithography
Abstract
The invention provides a novel rinsing fluid which can convert an easily wettable resist pattern surface having a contact angle of 40° or below into one having a contact angle of 70° or above to inhibit pattern collapse effectively and thereby give high-quality products. The rinsing fluid consists of a solution containing at least one fluorine compound soluble in water or alcoholic solvents which is selected from among compounds represented by the general formula (I), those represented by the general formula (II), and those represented by the general formula: R f ′—COOH: wherein R 1 and R 2 are each optionally substituted C 1-5 alkyl whose hydrogen atoms are partially or wholly replaced by fluorine, or R 1 and R 2 together with the SO 2 groups to which they are bonded and the nitrogen atom may form a five- or six-membered ring; R f is optionally substituted C 1-5 alkyl whose hydrogen atoms are partially or wholly replaced by fluorine; m and n are each an integer of 2 or 3; and R f ′ is at least partially fluorinated alkyl having 8 to 20 carbon atoms.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 12.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A rinse solution for lithography consisting essentially of a compound of the formula in a solvent which is a mixture of water and an alcoholic solvent.
- Claim 2Independent Claim
A rinse solution for lithography consisting essentially of a compound of the formula in a solvent which is a mixture of water and an alcoholic solvent.
- Claim 3Depends on #1
The rinse solution for lithography described in claim 1 wherein the ratio of water to alcoholic solvent is from 60:40 to 99:1 by volume.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (34)
Non-Patent Literature (2)
- Foropoulos et al., Nov. 1, 1984, Inorganic Chemistry, vol. 23, No. 23, pp. 3720-3723, "Method of Synthesizing a Sulfonimide represented by the formula of (CF.sub.3 SO.sub.2).sub.2 NH."
- Toshihiko Tanaka et al. "Mechanism of Resist Pattern Collapse During Development Process", Japan Appl. Phys., vol. 32 (1993), pp. 6059-6064.