A method of regeneration of a SCR catalyst for use in high temperature thermal processes such as in a power plant facility burning fossil fuels, bio-based fuels, or a combination thereof, wherein the catalyst is poisoned by phosphorous components in the flue gas and the catalyst is treated using a base, preferably an alkali metal hydroxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 17.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of regenerating a phosphorous-poisoned SCR catalyst, the method comprising treating the phosphorous-poisoned catalyst with an alkali metal hydroxide at a pH above 8.5.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the alkali metal hydroxide is sodium hydroxide, potassium hydroxide, or a combination thereof.

  3. Claim 3Independent Claim

    A method of regenerating a phosphorous-poisoned SCR catalyst, the method comprising treating the phosphorous-poisoned catalyst with an alkali metal hydroxide at a pH in a range of from above about 10 to about 14 and a temperature up to about 176° F.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 17 total)

PatentTitleYearCitations
US 9,228,468 B2Targeted regeneration of a catalyst in an aftertreatment system20167
US 8,268,743 B2Pluggage removal method for SCR catalysts and systems20127
US 10,471,384 B2System and method for reducing halogen levels necessary for mercury control, increasing the service life and/or catalytic activity of an SCR catalyst and/or control of multiple emissions20190
WO 2012/106195 A2Method for treating scr catalysts having accumulated iron compounds—1
US 8,691,719 B2System and method for increasing the service life and/or catalytic activity of an SCR catalyst and control of multiple emissions20141
US 8,389,431 B2Method for treating SCR catalysts having accumulated iron compounds20131
US 2011229388 A1System and method for increasing the service life and/or catalytic activity of an scr catalyst and control of multiple emissions—5
US 8,986,620 B2System for treating a platinum contaminated catalytic component20150
US 10,618,000 B2Coated articles having high kNOx/kSOx ratios for selective catalytic reduction20200
US 9,212,587 B2Exhaust throttle control for aftertreatment system thermal management20154
KR 20210049215 ASelective reduction catalyst for removing nitrogen oxide using ammonia, manufacturing method thereof and method for removing nitrogen oxide using the same—1
US 2018021724 A1COATED ARTICLES HAVING HIGH KNOx/KSOx RATIOS FOR SELECTIVE CATALYTIC REDUCTION—1
US 2010273643 A1System and method for protection of scr catalyst and control of multiple emissions—13
US 8,822,364 B2Method for treating a platinum contaminated catalytic component20145
US 10,213,738 B2System and method for increasing the service life and/or catalytic activity of an SCR catalyst and control of multiple emissions20191

Non-Patent Literature (5)

  • Differenzierung der Eisenoixde des Bodens durch Extraktion mit Ammoniumoxalat-Losung, Dr. Von U. Scwertmann May 3, 1964, pp. 194-202.
  • Emissions Control, SCR Maintenance Fundamentals, Ken Wicker and Jim Staudt, POWER, Jun. 2004, pp. 52-57.
  • JP 2007/297248 A (Hiroshi et al.) Nov. 15, 2007 Abstract.
  • JP 56037048 A (Kazutoyo et al.) Apr. 10, 1981 Abstract.
  • PCT International Search Report.