Method for cleaning a solar cell surface opening made with a solar etch paste

7Forward Citations (#15262622 Global)
0.4/yrCitation Velocity (#18282381 Global)
1.76Citation PageRank (#17856670 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A thin silicon solar cell having a back dielectric passivation and rear contact with local back surface field is described. Specifically, the solar cell may be fabricated from a crystalline silicon wafer having a thickness from 50 to 500 micrometers. A barrier layer and a dielectric layer are applied at least to the back surface of the silicon wafer to protect the silicon wafer from deformation when the rear contact is formed. At least one opening is made to the dielectric layer. An aluminum contact that provides a back surface field is formed in the opening and on the dielectric layer. The aluminum contact may be applied by screen printing an aluminum paste having from one to 12 atomic percent silicon and then applying a heat treatment at 750 degrees Celsius.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming a diffused layer on a doped substrate of a thin silicon wafer having a thickness from 50 to 200 micrometers, wherein the silicon wafer has a front surface and a back surface; forming a spin-on dielectric layer on the back surface of the silicon wafer; forming a barrier layer on the spin-on dielectric layer; applying an etch paste from one to 10 percent of the surface area of the barrier layer; applying a first heat treatment to the etch paste at a temperature from 300 to 380 degrees Celsius; and removing residue from an opening with a solution comprising hydrofluor

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the first heat treatment is applied for a time period from 30 to 45 seconds.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising: applying a contact paste to the back surface of the silicon wafer followi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,105,471 ASolar cell with improved printed contact and method of making the same197832
US 4,163,678 ASolar cell with improved N-region contact and method of forming the same197942
US 4,235,644 AThick film silver metallizations for silicon solar cells198063
US 4,442,310 APhotodetector having enhanced back reflection198499
US 5,011,782 AMethod of making passivated antireflective coating for photovoltaic cell199199
US 5,230,746 APhotovoltaic device having enhanced rear reflecting contact199368
US 5,468,652 AMethod of making a back contacted solar cell1995272
US 5,510,271 AProcesses for producing low cost, high efficiency silicon solar cells199651
WO 9,713,280 A1Self-aligned locally deep- diffused emitter solar cell—29
US 5,698,451 AMethod of fabricating contacts for solar cells199785
US 5,726,065 AMethod of preparing solar cell front contacts199896
US 5,766,964 AProcesses for producing low cost, high efficiency silicon solar cells199860
US 5,871,591 ASilicon solar cells made by a self-aligned, selective-emitter, plasma-etchback process1999102
US 5,899,704 ASolar cell with a back-surface field method of production199976
US 5,928,438 AStructure and fabrication process for self-aligned locally deep-diffused emitter (SALDE) solar cell1999203
EP 0,999,598 A1Solar cell and method for fabricating a solar cell—31
US 6,069,065 ASemiconductor device fabrication method200035
US 6,071,753 AMethod of producing a solar cell200043
US 6,091,021 ASilicon cells made by self-aligned selective-emitter plasma-etchback process2000181
US 6,093,882 AMethod of producing a solar cell; a solar cell and a method of producing a semiconductor device200080
US 6,096,968 ASolar cell with a back-surface field2000102
US 6,207,890 B1Photovoltaic element and method for manufacture thereof200190
US 6,291,763 B1Photoelectric conversion device and photo cell2001297

Non-Patent Literature (5)

  • International Search Report from corresponding PCT/US2008/005863 received Aug. 26, 2008.
  • International Search Report from PCT/US2008/005869 dated Jan. 28, 2009.
  • Office Action from U.S. Appl. No. 12/116,100 dated Oct. 1, 2009.
  • Rentsch J., et al. "Technology Route Towards Industrial Application of Rear Passivated Silicon Solar Cells," Photovoltaic Energy conversion, Conference Record of the 2006 IEEE 4th World Conference on, IEEE, PI, May 1, 2006, pp. 1008-1011, XP031007477, ISBN: 978-1-422-0016-4, p. 1008-1010; figure 1,
  • Schneiderlochner E., et al., "Investigations on Laser-Fired Contracts for Passivated Rear Solar Cells," 20020519; 20020519-20020524, vol. Conf. 29, May 19, 2002, pp. 300-303, XP010666288, Gelsenkirchen, Germany.