Patents
US 7,740,790 B2#13651484 Most CitedExpiredUnited States (USPTO)Utility

Method of making liquid crystal polymer films

8Forward Citations (#13651484 Global)
0.5/yrCitation Velocity (#15499014 Global)
1.68Citation PageRank (#19101235 Global)
36Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of making a thermotropic liquid crystal polymer film includes continuously heat treating of the thermotropic liquid crystal polymer film 2 while the latter is jointed to a sheet-like support member 4 , and subsequently separating the heat-treated thermotropic liquid crystal polymer film 2 from the support member 4 . The continuous heat treatment of the thermotropic liquid crystal polymer film 2 then jointed to the support member 4 is carried out for a predetermined heating time within the range of 5 to 60 seconds at a predetermined heating temperature T° C. equal to or higher than the melting point Tm° C. of the thermotropic liquid crystal polymer film less 15° C. (i.e., Tm−15° C.), but lower than the melting point Tm° C. (thus, Tm−15° C.≦T° C.<Tm° C.), to thereby increase the thermal expansion coefficient of the thermotropic liquid crystal polymer film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a thermotropic liquid crystal polymer film, which comprises: continuously heat treating an extruded thermotropic liquid crystal polymer film joined to a sheet-like support member; and subsequently separating the heat-treated thermotropic liquid crystal polymer film from the support member; wherein the continuous heat treatment of the thermotropic liquid crystal polymer film joined to the support member is carried out for a heating time of 5 to 60 seconds at a heating temperature T° C. equal to or higher than the melting point Tm° C. of the thermotropic liquid crystal polymer

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 4,717,624 AMethod of manufacturing a molded article having good dimensional stability198825
DE 3,625,263 A1Mikroelektronische bauelemente sowie dickschicht-hybridschaltungen—3
US 4,802,061 AMicroelectronic components and thick-film hybrid circuits198925
US 4,837,268 AWholly aromatic polyester198913
US 4,851,503 AWholly aromatic thermotropic liquid crystal polyester198912
US 4,863,767 AMethod of adhesive bonding by use of thermotropic liquid crystal polymers198928
US 4,975,312 AMultiaxially oriented thermotropic polymer substrate for printed wire board199059
US 4,983,318 AMethod for electric field orientation of liquid crystal polymers and oriented materials of liquid crystal polymers obtained by the method199145
US 5,091,138 AProduction of wholly aromatic polyester film19927
US 5,164,141 AProcess for the continuous production of laminated sheets199217
US 5,227,115 AProcess for aligning liquid-crystalline polymers199327
US 5,326,848 AThermotropic liquid crystal polyester199432
EP 0,604,838 A1Multiaxially reinforced liquid crystal polymer sheet—6
US 5,347,154 ALight valve device using semiconductive composite substrate199471
US 5,360,672 AProcess for treating film comprising liquid crystal polymer199424
US 5,460,748 ALiquid crystalline polymer film, process for producing same, and utilization thereof199539
US 5,529,740 AProcess for treating liquid crystal polymer film199651
US 5,601,884 ARetardation film and production thereof199740
US 5,688,436 AOptically anisotropic material, process for producing it, and retardation plate and liquid crystal display device using same199742
US 5,693,253 AOptically anisotropic material, process for producing it, and retardation plate and liquid crystal device using same199719
US 5,703,202 AProcess for treating liquid crystal polymer film199738
US 5,719,354 AMonolithic LCP polymer microelectronic wiring modules1998140

Non-Patent Literature (4)

  • Coefficient of Thermal Expansion (http://www.ami.ac.uk/courses/topics/0197-cte/index.html), retrieved Mar. 5, 2008.
  • Vectra® A950 product data sheet ( http://tools.ticona.com/tools/mcbasei/product-tools.php?sPolymer=LCP&sProduct=VECTRA) VECTRA® A presents a CTE of~4 ppm/oC-accessed Sep. 3, 2008.
  • Vectra® A950 product data sheet ( http://tools.ticona.com/tools/mcbasei/product-tools.php?sPolymer=LCP&sProduct=VECTRA) VECTRA® A presents a CTE of˜4 ppm/oC—accessed Sep. 3, 2008.
  • Vectra® E130i LCP Materials Data Property sheet (http://tools.ticona.com/tools/mcbasei/product-tools.php?sPolymer=LCP&sProduct=VECTRA), published Feb. 25, 2007.