A silicon wafer and a method for manufacturing the same are provided, wherein the silicon wafer has no crystal defects in the vicinity of the surface and provides excellent gettering efficiency in the process of manufacturing devices without IG treatment. The oxygen concentration and the carbon concentration are controlled respectively within a range of 11×10 17 -17×10 17 atoms/cm 3 (OLD ASTM) and within a range of 1×10 16 -15×10 16 atoms/cm 3 (NEW ASTM). A denuded zone having no crystal defects due to the existence of oxygen is formed on the surface and in the vicinity thereof, and oxygen precipitates are formed at a density of 1×10 4 -5×10 6 counts/cm 2 , when a heat treatment is carried out at a temperature of 500-1000° C. for 1 to 24 hours. In the method for manufacturing the silicon wafer, moreover, the silicon wafer having the oxygen and carbon concentrations as controlled above is heat-treated at a temperature of 1100° C.-1380° C. for 1 to 10 hours. The control of the oxygen and carbon concentrations in the growth of a single crystal with CZ method allows a desired density of oxygen precipitates to be attained in the process of manufacturing devices and thereby sufficient ge

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A silicon wafer in which the oxygen concentration and the carbon concentration are controlled respectively within a range of 11×10 17 -17×10 17 atoms/cm 3 (OLD ASTM) and within a range of more than 5×10 16 to 15×10 16 atoms/cm 3 (NEW ASTM), wherein a denuded zone having no crystal defects due to the existence of oxygen is formed on the surface and in the vicinity thereof, and wherein oxygen precipitates are formed at a density of 1×10 4 counts/cm 2 -5×10 6 counts/cm 2 , when a heat treatment is carried out at 500-1000° C. for 1 to 24 hours.

  2. Claim 2Depends on #1

    A silicon wafer according to claim 1 , wherein the thickness of said denuded zone is not less than 10 μm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.