hottubpatentshottub.tech
US 7,732,348 B2#174812 Most CitedActiveUnited States (USPTO)Utility

Method of producing a porous dielectric element and corresponding dielectric element

0Forward Citations (#174812 Global)
0.0/yrCitation Velocity (#174812 Global)
0.98Citation PageRank (#174812 Global)
10Prior Art Cited
13Structured Claims
0Drawings / Sheets

Abstract

A porous dielectric element is produced by forming a first dielectric and a second dielectric. The second dielectric is dispersed in the first dielectric. The second dielectric is then removed from the second dielectric by using a chemical dissolution. The removal of the second dielectric from the first dielectric leaves pores in the first dielectric. The pores, which are filled with air, improves the overall dielectric constant of the resulting dielectric element.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (13)

  1. Claim 1Independent Claim

    A method of producing a porous dielectric element, comprising: forming of at least a first dielectric and at least a second dielectric which is dispersed in the first dielectric, wherein the first dielectric is a dielectric formed by Si x C y H z ; and removing of the second dielectric by a chemical dissolution.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the porous dielectric element has a dielectric constant of 3.0 or less.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein the first dielectric is permeable to hydrofluoric acid and to the products of the dissolution of the second dielectric by hydrofluoric acid, and wherein removing the second dielectric comprises dissolving the second dielectric by a fluid containing hydrofluoric acid.

  4. Claim 4Depends on #3

    The method according to claim 3 , wherein the fluid containing hydrofluoric acid comprises at least one of the compounds chosen from the group formed by: liquid hydrofluoric acid, gaseous hydrofluoric acid and hydrofluoric acid diluted in supercritical carbon dioxide.

  5. Claim 5Depends on #3

    The method according to claim 3 , wherein the second dielectric contains silicon-oxygen bonds.

  6. Claim 6Depends on #5

    The method according to claim 5 , wherein the second dielectric comprises at least one of the materials chosen from the group formed by: SiO 2 , Si w O x C y H z and siloxanes.

  7. Claim 7Depends on #1

    The method according to claim 1 , wherein the proportion by volume of the second dielectric in the formation of the first dielectric and of the second dielectric is between 10% and 40%.

  8. Claim 8Depends on #1

    The method according to claim 1 , wherein forming comprises performing plasma-enhanced chemical vapor deposition using a first-type organosilicon precursor for forming the first dielectric and using a second-type organosilicon precursor for forming the second dielectric, wherein the second dielectric is uniformly dispersed within the first dielectric.

  9. Claim 9Depends on #1

    The method according to claim 1 , wherein forming comprises performing spin-on deposition of the first dielectric mixed with molecules which comprise the second dielectric.

  10. Claim 10Depends on #1

    The method according to claim 1 , wherein forming comprises using a material for the second dielectric, which is dispersed within the first dielectric, that includes silicon-oxygen bonds and wherein removing comprises attacking the silicon-oxygen bonds of the second dielectric material by chemical dissolution.

  11. Claim 11Independent Claim

    A method of producing a porous dielectric element, comprising: forming of at least a first dielectric and at least a second dielectric which is dispersed in the first dielectric; and removing of the second dielectric by a chemical dissolution; wherein forming comprises performing plasma-enhanced chemical vapor deposition using a first-type organosilicon precursor for forming the first dielectric and using a second-type organosilicon precursor for forming the second dielectric, wherein the second dielectric is uniformly dispersed within the first dielectric; and wherein the first-type organosilicon precursor is of Si x C y H z type and the second-type organosilicon precursor is of Si w O x C y H z type.

  12. Claim 12Depends on #11

    The method according to claim 11 , wherein the Si x C y H z type is dimethylphenylsilane and the Si w O x C y H z type is tetraethylorthosilicate.

  13. Claim 13Independent Claim

    A method of producing a porous dielectric element, comprising: forming of at least a first dielectric and at least a second dielectric which is dispersed in the first dielectric; and removing of the second dielectric by a chemical dissolution; wherein forming comprises performing spin-on deposition of the first dielectric mixed with molecules which comprise the second dielectric; wherein the first dielectric is SiLK material and the second dielectric comprises siloxane molecules; and wherein the SiLK material does not contain any silicon atoms and the siloxane is of the decamethylc

Technical Overview & Description

PRIORITY CLAIM The present application is a translation of and claims priority from French Application for Patent No. 06 55558 of the same title filed Dec. 15, 2006, the disclosure of which is hereby incorporated by reference. BACKGROUND OF THE INVENTION 1. Technical Field of the Invention The present invention relates to dielectric elements, especially but not exclusively to porous dielectric elements having a low dielectric constant, which are intended, for example, to be incorporated into integrated circuits. 2. Description of Related Art To reduce information propagation times in the interconnects (metal lines, vias, etc.) of integrated circuits, it is beneficial to use materials having a low dielectric constant (or relative permittivity), typically of less than 4.0, in order to isolate these metal interconnects. In addition, a material having a low dielectric constant promotes decoupling between the various lines. One way of decreasing the dielectric constant of a dielectric is to produce it in porous form. This is because the presence in the pores of gas, the dielectric constant of which, equal to 1, is the lowest possible, makes it possible to reduce the overall dielectric constant of the porous material. A known method of producing a porous material consists in producing a hybrid material comprising, on the one hand, an Si w O x C y H z matrix and, on the other hand, nanoscale organic inclusions and then in degrading, by a heat treatment alone or a heat treatment enhanced by ultraviolet radiation or by an electron beam, the organic inclusions so as to obtain the final porous material. SUMMARY OF THE INVENTION According to one mode of implementation, a method is presented for producing a porous dielectric that requires no heat treatment step. According to a first aspect, what is proposed is a method of producing a porous dielectric element, comprising: a) forming at least a first dielectric and at least a second di

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (10)

PatentTitleYearCitations

Non-Patent Literature (3)

  • Favennec, et al., "Porous extreme low kappa (ELkappa) dielectrics using a PECVD porogen approach;" Materials Science in Semiconductor Processing, Elsevier Science Publishers, B.V., Barking, UK, vol. 7, No. 4-6, 2004, pp. 277-282, XP004639152; ISSN: 1369-8001.
  • Preliminary French Search Report, FR 06 55558, dated Sep. 26, 2007.
  • Preliminary French Search Report, FR 07 59356, dated Mar. 5, 2008.