Polyolefin masterbatch and composition suitable for injection molding
Abstract
A masterbatch composition comprising (percent by weight): A) 15%-50% of a polypropylene component having a melt flow rate of from 1 to 250 g/10 min.; and B) 50%-85% of an olefin polymer partially soluble in xylene at room temperature, containing from 60% to 85% by weight of ethylene; said masterbatch composition having (i) a value of the intrinsic viscosity [η] of the fraction soluble in xylene at room temperature ([η] sol ) equal to or lower than 2.9 dl/g, and (ii) a value of the ratio MFR/[η], , , , equal to or lower than 4, is added to polyolefin materials to obtain final compositions suitable for injection molding.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A masterbatch composition comprising (percent by weight): A) 15%-50% of a crystalline propylene homopolymer having a melt flow rate of from 1 to 250 g/10 min.; and B) 50%-85% of an olefin polymer partially soluble in xylene at room temperature comprising from 55% to 85% by weight of ethylene; said masterbatch composition having an intrinsic viscosity [η] of a fraction soluble in xylene at room temperature ([η] sol ) equal to or lower than 2.7 dl/g, and a ratio of MFR/[η] sol value equal to or lower than 4, wherein the MFR is the melt flow rate of the masterbatch composition.
- Claim 2Depends on #1
The masterbatch composition of claim 1 further having a MFR value of from 0.1 to 15 g/10 min.
- Claim 3Depends on #1
The masterbatch composition of claim 1 further having a flexural modulus value ranging from 255 MPa to 400 MPa.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗