US 7,722,918 B2#24835807 Most CitedActiveUnited States (USPTO)Utility

Process for the preparation of high temperature superconducting bulk current leads with improved properties and superconducting bulk current leads made thereby

4Forward Citations (#24835807 Global)
0.2/yrCitation Velocity (#28461844 Global)
1.37Citation PageRank (#26301023 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a process for the preparation of high temperature superconducting (HTS) bulk current leads capable of supplying a continuous current of more than 200 A at 77 K, at least for 2 to 4 hours without any substantial heat load to cryogen free cryocooler and other superconducting magnet systems. The superconducting bulk current leads with improved properties are prepared from an improved high temperature superconducting (HTS) bismuth based cuperate [(Bi, Pb) 2 Sr 2 Ca 2 Cu 3 O 10+x ] material in tube and rod shape with both end metallic contacts. To produce such a lead, the process included modification of the superconducting material with homogeneous silver addition, a step of initial sintering in a large size tube followed by crushing into powder, a step of shaping the said initially sintered tube powder into tubes and rods of different size, a step of formation of metallic contacts by a perforated silver foil sandwiched between two metal spray deposited silver at both end parts of the said tubes and rods followed by a final step of co-sintering. In the current leads obtained according to these aspects, it is possible to stably carry current more than 200

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of high temperature superconducting (HTS) bulk current leads with improved properties, which comprises the steps of: (i) preparing separate water-based solutions of nitrates of Bi, Pb, Sr, Ca and Cu in molar ratio in the range of 1.74 to 1.84:0.34 to 0.4:1.83 to 2.0:1.97 to 2.2:3.0 to 3.13 and then mixing the solutions together to form a single solution; (ii) adding silver in molar ratio of 0.06 to 1.8 in the form of a water-based silver nitrate solution in the single solution (i) to obtain a resultant nitrate solution; (iii) spray drying the resultant nitrate sol