Method for welding two welding parts by means of a fillet weld and welding part with an inclined tapered edge area therefor
Abstract
The invention relates to a method for welding two welding parts ( 1, 3 ) by means of a fillet weld ( 11 ), wherein a first welding part ( 1 ), with a bearing surface at least in an edge area of an edge that is to be welded by means of a fillet weld, is brought into contact with a bearing surface of a welding part ( 3 ) and the welding energy ( 5 ) is supplied in an energy supply area during the welding process, exclusive of a surface ( 7 ) of the first welding part facing away from the bearing surface, said energy supply area being located at a predetermined distance from the edge of the first welding part. The welding energy is supplied in a direction, whereby the direction component thereof points perpendicular to the course of the fillet weld that is to be produced in the direction of an inner area of the first welding part, forming a welding angle of less than 90° with the contact plane of the bearing surfaces of the first and second welding parts. The welding energy is supplied until at least the energy supply area of the first welding part and a sufficient area of the second part, which is adjacent to the energy supply area of the first welding part, and also the material sup
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A welding part for welding to a second welding part by means of a fillet weld ( 11 ), wherein: a first welding part ( 1 ) has a bearing surface which, at least in an edge area, can be brought into contact with a bearing surface of a second welding part ( 3 ) to be welded by means of a fillet weld ( 11 ), the edge area of the first welding part ( 1 ) has an energy supply area for the supply of welding energy on one of the bearing surfaces turned away from the surface of the first welding part ( 1 ), the edge area has a structure ( 9 ′) which is favorable to the supply of energy for producing th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.