US 7,713,795 B2#40066723 Most CitedActiveUnited States (USPTO)Utility

Flash memory device with single-poly structure and method for manufacturing the same

2Forward Citations (#40066723 Global)
0.1/yrCitation Velocity (#41635180 Global)
1.01Citation PageRank (#41095080 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A flash memory device has a single-poly structure. A method for manufacturing the flash device includes forming an oxide layer over a semiconductor substrate having a P-well region or N-well region. A shallow trench isolation (STI) may be formed in the semiconductor substrate and the oxide layer. A drift region may be formed by injecting a dopant into a part of the P-well region or N-well region. A gate oxide layer and a poly-silicon layer may be formed over the well region, the drift region, and the STI. A control gate pattern may be formed by patterning the gate oxide layer and the poly-silicon layer. A source region and a drain region may be formed on opposite sides of the control gate pattern. A silicon nitride layer may be deposited over the control gate pattern and etching the silicon nitride layer to form a spacer around a sidewall of the control gate pattern. A plurality of insulating layers may be formed over the control gate pattern, and via-patterns may be electrically connected to the source region and the drain region, respectively. A drain electrode and a source electrode may be electrically connected to the via-patterns, respectively.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming an oxide layer over a semiconductor substrate having a well region; forming a shallow trench isolation in the semiconductor substrata and the oxide layer; forming a drift region by injecting a dopant into a part of the well region; sequentially forming a gate oxide layer and a poly-silicon layer over the well region, the drift region, and the shallow trench isolation; forming a control gate pattern by patterning the gate oxide layer and the poly-silicon layer; forming a source region and a drain region at opposite sides of the control gate pattern; depositing a sil

  2. Claim 2Depends on #1

    The method of claim 1 , wherein, in the formation of the control gate pattern, the poly-silicon layer is a single l

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗