Patents
US 7,709,415 B2#9041037 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing activated carbon, polarizable electrode, and electric double-layered capacitor

11Forward Citations (#9041037 Global)
0.7/yrCitation Velocity (#11050745 Global)
2.79Citation PageRank (#8512978 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Activated carbon useful as polarizable electrode material for an electric double-layer capacitor can be obtained by mixing a carbonaceous material and an alkali metal hydroxide while maintaining a solid state, granulating the obtained mixture while maintaining its solid state, dehydrating the obtained granulated substance while maintaining its solid state, and subjecting the granulated dehydration product obtained in the dehydration step to an activation treatment. The preferred pressure of the granulation treatment in the granulation step is 0.01 to 300 Torr, and the preferred temperature of the granulation treatment is 90 to 140° C. The preferred pressure of the dehydration treatment in the dehydration step is 0.01 to 10 Torr, and the preferred temperature of the dehydration treatment is 200 to 400° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 11.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an activated carbon, comprising: mixing a carbonaceous material and an alkali metal hydroxide while maintaining a solid state to obtain a mixture; granulating the mixture while maintaining a solid state to obtain a granulated product; dehydrating the granulated product while maintaining a solid state to obtain a dehydrated product; and subjecting the dehydrated product to an activation treatment to obtain the activated carbon, wherein the carbonaceous material comprises grains with a maximum length of 500 μm or less in the direction of the major axis.

  2. Claim 2Depends on #1

    The manufacturing method according to claim 1 , wherein the temperature in said granulating is 80° C. or more.

  3. Claim 3Depends on #1

    The manufacturing method according to claim 1 , wherein the maximum diameter of the granulated product is 50 mm or less. 4

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 3,539,467 AHot briquetting and oxidation of coal-pitch mixtures in preparing activated carbon197039
US 4,159,306 AApparatus for the production of activated carbon197917
US 4,612,689 AMethod of manufacturing multilayer capacitors198621
JP S6261529 AConcrete block—4
US 5,446,005 APitch-based activated carbon fiber199547
US 5,540,974 AMetallized polyester film capacitor199626
US 5,646,815 AElectrochemical capacitor with electrode and electrolyte layers having the same polymer and solvent199752
JP H10199767 AManufacture of carbon material for electric double layer capacitor—33
US 5,891,822 AProduction process of active carbon used for electrode for organic solvent type electric double layer capacitor199936
US 5,956,225 AActivated carbon, process for the preparation thereof and electric double layer-type capacitor electrode199961
JP H11293527 AOptically isotropic pitch-based activated carbon fiber and electric double layer capacitor using the same—10
JP H11349320 AProduction of activated carbon—15
US 6,118,650 AMesophase pitch-based activated carbon fibers and electric double layer capacitor using the same200042
WO 0,078,138 A2Method for producing shaped, activated charcoal—6
JP 2001019415 AMethod and device for alkali recycle regeneration of carbon material—8
WO 0,113,390 A1Method for producing activated carbon for electrode of electric double-layer capacitor—7
EP 1,103,523 A2Activated carbon and method for producing it—8
EP 1,176,617 A2Activated carbon, process for producing the same, polarizable electrode, and electric double layer capacitor—12
CN 1,334,237 AActive carbon and its production method, polarizable electrode and double layer capacitor—18

Non-Patent Literature (2)

  • Machine translation of JP 11-293527.
  • Otowa, et al., Development of KOH Activated High Surface Area Carbon and its Application to Drinking Water Purification, Carbon 1997; 35(9): 1315-1317.