Method for producing a ballistic protective armour

1Forward Citations (#55850283 Global)
0.1/yrCitation Velocity (#52753449 Global)
0.80Citation PageRank (#55850283 Global)
16Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for producing a ballistic protective armour includes superimposing a certain number of textile layers ( 116 ) in such a way that a layer structure ( 114 ) is formed, in sewing the textile layers ( 116 ) of the layer structure to each other and in pressing the layer structure ( 114 ). Prior to a sewing process, the textile layers ( 116 ) of the layer structure ( 114 ) are pre-pressed by a pre-pressing process ( 30 ) in such a way that a preform ( 130 ), whose three-dimensional shape corresponds to a final product shape, is formed and subsequently, after the sewing process ( 50 ), the preform is exposed to a heat-pressing process ( 100 ) at a temperature greater than the temperature of the pre-pressing process ( 30 ).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method for producing a ballistic protective armor comprising the following steps: layering a number of textile layers onto each other to form a layered structure, sewing the textile layers of the layered structure together, and pressing the layered structure, including the steps of: pre-pressing the textile layers of the layered structure in a cold press comprising a lower hemispherical mold half and an upper hemispherical mold half before sewing in a pre-pressing step to form a hemispherical preform with a shape corresponding to an end product to be produced, and hot pressing said preform in

  2. Claim 2Depends on #1

    Method according to claim 1 , wherein the temperature during the hot pressing step lies in the range between 150° C. and 175° C.

  3. Claim 3Independent Claim

    Method accord

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗