Method and device for the production of a silicon single crystal, silicon single crystal, and silicon semiconductor wafers with determined defect distributions

0Forward Citations (#96711669 Global)
0.0/yrCitation Velocity (#96711669 Global)
0.56Citation PageRank (#96711669 Global)
28Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for the production of a silicon single crystal by pulling the single crystal, according to the Czochralski method, from a melt which is held in a rotating crucible, the single crystal growing at a growth front, heat being deliberately supplied to the center of the growth front by a heat flux directed at the growth front. The method produces a silicon single crystal with an oxygen content of from 4*10 17 cm −3 to 7.2*10 17 cm −3 and a radial concentration change for boron or phosphorus of less than 5%, which has no agglomerated self-point defects. Semiconductor wafers are separated from the single crystal. These semiconductor wafers have may have agglomerated vacancy defects (COPs) as the only self-point defect type or may have certain other defect distributions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for the production of a silicon single crystal comprising pulling the single crystal, according to the Czochralski method, from a melt which is held in a rotating crucible, the single crystal growing at a growth front having a center region and an edge region; iso-rotating the single crystal and the crucible; providing a heat source arrayed at the center of the bottom of the crucible; supplying heat to the center of the growth front by the heat source acting on the center of the growth front, so that per unit time, more heat reaches the center region of the growth front than the edge

  2. Claim 2Depends on #1

    The method of claim 1 , wherein a curvature of the growth front is reduced or increased.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein an axial temperature gradient G(r) at the growth front is regulated, r ex

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (28)

PatentTitleYearCitations
US 3,551,115 AApparatus for growing single crystals197023
JP S61178490 AHeater for single crystal pulling up apparatus—4
JP H0416591 ASingle crystal pulling up device for compound semiconductor—2
US 5,162,072 AApparatus and method for control of melt flow pattern in a crystal growth process199242
US 5,567,399 AApparatus for producing a single crystal199656
US 5,997,635 AMethod for fabricating a single-crystal semiconductor199922
KR 20000005835 ASilicon Single Crystal Wafer and Method for Producing Silicon Single Crystal Wafer—2
US 6,086,671 AMethod for growing a silicon single crystal200023
US 6,113,688 AProcess for producing single crystals200032
US 6,153,008 ADevice and method for pulling a single crystal200040
US 6,190,631 B1Low defect density, ideal oxygen precipitating silicon200138
JP 2001199793 ASingle crystal pull device—2
JP 2001261495 AMethod for producing defect-free crystal—17
US 6,299,982 B1Silicon single crystal wafer and method for producing silicon single crystal wafer200125
US 2001047749 A1Apparatus and method of growing single crystal of semiconductor—5
US 2002048670 A1Single crystalline silicon wafer, ingot and producing method thereof—5
US 2002081440 A1Silicon wafer and epitaxial silicon wafer utilizing same—38
US 6,413,310 B1Method for producing silicon single crystal wafer and silicon single crystal wafer200243
US 6,416,836 B1Thermally annealed, low defect density single crystal silicon200214
US 2002092461 A1Process and apparatus for producing a silicon single crystal—18
JP 2002249396 AMethod for growing silicon single crystal—6
EP 1,270,769 A1Method for producing silicon single crystal having no flaw—6
US 6,569,535 B2Silicon wafer and epitaxial silicon wafer utilizing same200320
US 2003106485 A1High resistivity silicon wafer and method of producing same using the magnetic field czochralski method—9
US 2003172865 A1Silicon single crystal wafer having void denuded zone on the surface and diameter of above 300mm and its production method—10
JP 2004143002 AApparatus and method for controlling silicon melt convection—2
US 6,869,478 B2Method for producing silicon single crystal having no flaw200528
US 7,235,133 B2Method for growing single crystal of semiconductor20073

Non-Patent Literature (5)

  • Ammon. Journal of Crystal Growth, 151, 1995, pp. 273-277.
  • Eidenzon/Puzanov in Inorganic Materials, vol. 33, No. 3, 1997, pp. 219-255.
  • English Abstract corresponding to JP 2001199793.
  • English Abstract corresponding to JP 2002249396.
  • English Abstract corresponding to JP 2004-143002.