Patents
US 7,700,009 B2#61943229 Most CitedActiveUnited States (USPTO)Utility

Method for producing positive electrode active material of non-aqueous electrolyte secondary cell

1Forward Citations (#61943229 Global)
0.1/yrCitation Velocity (#53054139 Global)
0.74Citation PageRank (#61943229 Global)
29Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for producing a positive electrode active material that realizes a non-aqueous electrolyte secondary cell having high discharge capacity and excellent high temperature preservation characteristic is provided. The method includes: an underwater kneading step of kneading lithium nickel composite oxide (Li x Ni 1-y M y O z , 0.9<x≦1.1, 0≦y≦0.7, 1.9≦z≦2.1, M including at least one selected from Al, Co, and Mn), lithium iron phosphorus composite oxide (LiFePO 4 ), a conductive carbon source, and water; after the underwater kneading step, a cleaning step of removing the water from the mixture after the underwater kneading step; and after the cleaning step, a baking step of baking the mixture in a reduced atmosphere at 200 to 800° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a positive electrode active material for a non-aqueous electrolyte secondary cell, the method comprising: an underwater kneading step of kneading lithium nickel composite oxide (Li x Ni 1-y M y O z , 0.9<x≦1.1, 0≦y≦0.7, 1.9≦z≦2.1, M including at least one selected from Al, Co, and Mn), lithium iron phosphorus composite oxide (LiFePO 4 ), a conductive carbon source, and water; a cleaning step of removing the water and an alkaline component remaining on the surface of the lithium nickel composite oxide from the mixture after the underwater kneading step; and a baking st

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the lithium iron phosphorus composite oxide is 1 to 20 mass % relative to the lithium nickel composite oxide.

  3. Claim 3Independent Claim

    The method according to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
JP 2001307730 APositive electrode and nonaqueous electrolyte battery—21
US 2002004169 A1Positive electrode and non-aqueous electrolyte cell—66
US 6,344,294 B1Process for preparing a positive electrode active material for a nonaqueous secondary battery by forming an oxalate precipitate200212
JP 2002075368 APositive electrode active material, nonaqueous electrolyte battery, and their manufacturing method—44
US 6,379,644 B2Process for producing a positive electrode active material for a nonaqueous secondary battery and a nonaqueous secondary battery using the active material20022
US 2003124423 A1Lithium secondary battery—55
JP 2003292308 ACarbon composite of lithium/iron/phosphorus-based complex oxide, production method therefor, positive pole activating material for lithium secondary battery, and lithium secondary battery—63
US 2003211235 A1Method of preparing positive active material for a lithium secondary battery—40
US 2003215717 A1Battery—50
JP 2004087299 APositive electrode active material and nonaqueous electrolyte secondary battery—62
US 6,720,113 B2Solid electrolyte cell200424
US 2004096743 A1Positive active material and non-aqueous electrolyte secondary battery—85
US 2004151980 A1Cell—5
US 2004253518 A1Positive active material and nonaqueous electrolyte secondary battery produced using the same—47
US 2005048371 A1Non-aqueous electrolyte secondary battery—28
JP 2005123107 AActive material for electrochemical element, its manufacturing method, and the electrochemical element using the same—80
JP 2005183384 AElectrochemical active material for positive electrode of lithium rechargeable electrochemical cell—7
US 2005196673 A1Electrochemically active material for the positive electrode of a lithium rechargeable electrochemical cell—23
JP 2005276475 APositive electrode material for lithium battery, electrode for lithium battery, and lithium battery—2
US 2006099495 A1Cathode and battery—76
JP 2006134770 ACathode and battery—36
US 2006153972 A1Method of manufacturing electrode for electrochemical device—24
US 2006194114 A1Positive electrode active material for non-aqueous electrolyte secondary battery, manufacturing method thereof, and non-aqueous electrolyte secondary battery using the positive electrode active material—47
US 2006216601 A1Cathode material and battery—23
US 2007212611 A1Lithium secondary battery—7
JP 4,061,586 B2非水電解質二次電池用正極活物質及びそれを用いた非水電解質二次電池20081
US 2008096109 A1Composition For Electrode, Electrode And Battery—17
US 2009029255 A1Secondary-battery current collector, secondary-battery cathode, secondary-battery anode, secondary battery and production method thereof—29
US 2009095942 A1Positive Electrode Material for Lithium Secondary Battery—21