Patents
US 7,696,299 B2#75242040 Most CitedActiveUnited States (USPTO)Utility

Fast crystallizing modified polyethylene naphthalate

0Forward Citations (#75242040 Global)
0.0/yrCitation Velocity (#75242040 Global)
0.56Citation PageRank (#75242040 Global)
19Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to modified Polyethylene Naphthalate (PEN) polymers with fast crystallizing properties, which helps in crystallization of amorphous PEN resin prior to its solid state polymerization (SSP).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making a rapidly crystallizable amorphous polyethylene naphthalate (PEN) polymer, the method comprising the steps of: (a) transesterifying dimethyl 2,6-naphthalene dicarboxylate (NDC) in the presence of (i) monoethylene glycol (MEG); (ii) at least one transesterification catalyst; and (iii) at least one nucleating agent, wherein about 80% of the transesterifying step is carried out at about 1050 mbar followed by about 20% of the transesterifying step being carried out at about 500 mbar, to form a prepolymer; and (b) polymerizing the prepolymer at about 250° C. to about 305° C. in t

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein about 80% of the transesterifying step is carried out at atmospheric pressure.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein about 20

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 4,798,883 AModified polyethylene naphthalate198910
US 4,963,644 AProcess for crystallization of polyethylene naphthalate199037
US 5,157,168 AProcess for the production of fatty alcohols199245
US 5,356,972 ANucleating agents for poly(ethylene terephthalate)199423
US 5,391,694 ASolid state polymerization of polyesters with low diffusion resistance prepolymer granules199518
US 5,412,063 ASolid state polymerization of polyesters with low diffusion resistance prepolymer granules19959
US 5,523,361 AProcess for crystallizing polyethylene naphthalate199616
US 5,594,092 AProcess for manufacturing polyester copolymers199715
US 5,612,423 AProcess for manufacturing polyester copolymers containing terephthalate and naphthalate units199711
US 5,714,571 AProcess for the crystallization of polyester resins199834
US 5,723,520 APolyester molding compositions and articles exhibiting good impact, heat and solvent resistance199836
US 5,744,578 AProcess for the crystallization of polyethylene naphthalate prepolymers and the solid stating of those crystallized prepolymers199823
US 5,750,644 AProcess for the crystallization of polyethylene naphthalate prepolymers and the solid stating of those crystallized prepolymers199820
US 5,895,807 AProcess for manufacturing polyester copolymers199919
US 6,124,423 AProcess for crystallizing polyethylene naphthalate copolymers in the absence of devolatilization20003
US 6,300,462 B1Process for preparing poly(ethylene-2,6-naphthalene dicarboxylate20019
US 2002168509 A1Nano-and micro-cellular foamed thin-walled material, and processes and apparatuses for making the same—47
US 6,663,961 B2Process for preparation of polyester-based polymers200310
US 6,749,785 B2Multilayer structures of poly(1,3-propylene 2,6 napthalate) and poly (ethylene terephthalate)200421